AKROLOY®

Preliminary

PARA GF 35 FR natural (8038)

PARA GF35 FR(40)

AKROLOY® PARA GF 35 FR natural (8038) - PARA, 35% GF, highest modulus and strength, flame retardant, very good flowability, good surface, low creep.


Modulus

14.500MPa

Strength

190MPa

Impact

50kJ/m²

AKROLOY® PARA GF 35 FR natural (8038) - PARA, 35% GF, highest modulus and strength, flame retardant, very good flowability, good surface, low creep.

AKROMID®

UL
Preliminary

A3 GF 30 8 HU black (8112)

PA66 GF30

AKROMID® A3 GF 30 8 HU black (8112) - PA 6.6, 30% glass fibre, heat ageing resistant, high rigidity and strength, UL HB all colors listed, NSF 61, WRAS, EU10/2011


Modulus

10.500MPa

Strength

200MPa

Impact

75kJ/m²

AKROMID® A3 GF 30 8 HU black (8112) - PA 6.6, 30% glass fibre, heat ageing resistant, high rigidity and strength, UL HB all colors listed, NSF 61, WRAS, EU10/2011

AKROMID®

UL

B3 GF 30 FR natural (7458)

PA6 GF30 FR(40)

AKROMID® B3 GF 30 FR natural (7458) is a 30% glass fibre reinforced, halogene free flame retardant polyamide 6 with flammability acc UL 94 V0 and low corrosion.


Modulus

10.800MPa

Strength

135MPa

Impact

65kJ/m²

AKROMID® B3 GF 30 FR natural (7458) is a 30% glass fibre reinforced, halogene free flame retardant polyamide 6 with flammability acc UL 94 V0 and low corrosion.

AKROLOY®

Preliminary

PARA GF 35 FR orange (8039)

PARA GF35 FR(40)

AKROLOY® PARA GF 35 FR orange (8039) - PARA, 35% GF, highest modulus and strength, flame retardant, very good flowability, good surface, low creep, RAL 2003.


Modulus

14.500MPa

Strength

190MPa

Impact

50kJ/m²

AKROLOY® PARA GF 35 FR orange (8039) - PARA, 35% GF, highest modulus and strength, flame retardant, very good flowability, good surface, low creep, RAL 2003.

AKROMID®

UL

A3 GF 30 8 HU natural (8102)

PA66 GF30

AKROMID® A3 GF 30 8 HU natural (8102) - PA 6.6, 30% glass fibre, heat ageing resistant, high rigidity and strength, UL HB all colors listed, NSF 61, WRAS, EU10/2011


Modulus

10.500MPa

Strength

200MPa

Impact

75kJ/m²

AKROMID® A3 GF 30 8 HU natural (8102) - PA 6.6, 30% glass fibre, heat ageing resistant, high rigidity and strength, UL HB all colors listed, NSF 61, WRAS, EU10/2011

AKROTEK®

RA GFM 15/25 black (8216)

PA6 (GF15+MD25)

AKROTEK® RA GFM 15/25 black (8216) - PA 6, 15% glass fiber reinforced, 25% mineral filled, radar absorption, 76-81 GHz


Modulus

8.500MPa

Strength

120MPa

Impact

50kJ/m²

AKROTEK® RA GFM 15/25 black (8216) - PA 6, 15% glass fiber reinforced, 25% mineral filled, radar absorption, 76-81 GHz

AKROMID®

C28 GF 25 FRT natural (7332)

PA-Blend

C28 GF 25 FRT natural (7332) - PA blend, 25% glass fiber, flame retardant, good flowability, Public Transportation EN 45545-2.


Modulus

10.800MPa

Strength

157MPa

Impact

64kJ/m²

C28 GF 25 FRT natural (7332) - PA blend, 25% glass fiber, flame retardant, good flowability, Public Transportation EN 45545-2.

112131480

AKROMID®

A3 GF 50 4 black (7282)PA66 GF50

AKROMID® A3 GF 50 4 black (7282) is a 50% glass fibre reinforced, hydrolysis/chemical stabilised polyamide 6.6 with very high rigidity and strength

Features

heat stabilised 160
hydrolysis / chemically stabilised

Properties

Modulus

17.000MPa

Strength

250MPa

Impact

110kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
17000 MPa
13000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
250 MPa
180 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
3,0 %
4,0 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
15500 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
380 MPa

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
110 kJ/m²
115 kJ/m²
110 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
20 kJ/m²
25 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
260 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
262 °C

Temperature index for 50% loss of tensile strength

IEC 60216

5.000 h
160 °C

General properties


Density

ISO 1183

23°C
1,57 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
1,3 - 1,5 %

Water absorption

ISO 62

23°C, saturated
3,7 - 4,3 %

Molding shrinkage

ISO 294-4

flow
transverse
0,1 - 0,3 %
0,5 - 0,7 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more