AKROLOY®

PA GF 50 natural (6414)

PA66+PA6I/6T GF50

AKROLOY® PA GF 50 natural (6414) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.


Modulus

17.000MPa

Strength

275MPa

Impact

110kJ/m²

AKROLOY® PA GF 50 natural (6414) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.

AKROMID®

T5 GF 35 4 black (7692)

PPA GF35

AKROMID® T5 GF 35 4 black (7692) is a 35% glass fibre reinforced polyphthalamide with inorganic heat stabilization, very high rigidity and strength, designed for hydrolysis resistance. This aromatic PPA keeps mechanical performance even at elevated temperatures or moisture pic-up


Modulus

13.500MPa

Strength

220MPa

Impact

70kJ/m²

AKROMID® T5 GF 35 4 black (7692) is a 35% glass fibre reinforced polyphthalamide with inorganic heat stabilization, very high rigidity and strength, designed for hydrolysis resistance. This aromatic PPA keeps mechanical performance even at elevated temperatures or moisture pic-up

AKROMID®

Preliminary

T9 GF 50 black (7601)

PPA GF50

AKROMID® T9 GF 50 black (7601) is a 50% glass fibre reinforced partially aromatic polyphthalamide with very high stiffness and strength, as well as high temperature and chemical resistance. The compound is based on PA9T and has lower moisture uptake than conventional PA6T variants. This leads to a significantly higher consistency of the glass transition temperature and higher strength at elevated temperatures especially in conditioned state.


Modulus

17.000MPa

Strength

250MPa

Impact

95kJ/m²

AKROMID® T9 GF 50 black (7601) is a 50% glass fibre reinforced partially aromatic polyphthalamide with very high stiffness and strength, as well as high temperature and chemical resistance. The compound is based on PA9T and has lower moisture uptake than conventional PA6T variants. This leads to a significantly higher consistency of the glass transition temperature and higher strength at elevated temperatures especially in conditioned state.

AKROMID®

A3 GM 20/10 4 WIT black (4529)

PA66 (GF20+GB10)

AKROMID® A3 GM 20/10 4 WIT black (4529) - 20% glass fibre, 10% glass bead, hydrolysis/chemical, polyamide 6.6, good surface, low warpage


Modulus

8.200MPa

Strength

175MPa

Impact

65kJ/m²

AKROMID® A3 GM 20/10 4 WIT black (4529) - 20% glass fibre, 10% glass bead, hydrolysis/chemical, polyamide 6.6, good surface, low warpage

AKROMID®

D3 GF 30 1 black (5392)

PA612 GF30

AKROMID® D3 GF 30 1 black (5392) - PA 6.12, 30% glass fiber, connector


Modulus

9.500MPa

Strength

180MPa

Impact

95kJ/m²

AKROMID® D3 GF 30 1 black (5392) - PA 6.12, 30% glass fiber, connector

AKROMID®

A28 LGF 50 9 black (7705)

PA66 LGF50

AKROMID® A28 LGF 50 9 black (7705) - 50% long glass fiber reinforced PA6.6, easy flowing, process improved, low shrinkage, very good fatigue performance, oil pan


Modulus

18.000MPa

Strength

270MPa

Impact

95kJ/m²

AKROMID® A28 LGF 50 9 black (7705) - 50% long glass fiber reinforced PA6.6, easy flowing, process improved, low shrinkage, very good fatigue performance, oil pan

AKROTEK®

PK-VM natural (4774)

PK

AKROTEK® PK-VM natural (4774) - Polyketon, Tribology, friction and wear, chemical resistance


Modulus

1.500MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-VM natural (4774) - Polyketon, Tribology, friction and wear, chemical resistance

1891080

AKROTEK®

Preliminary

PK-VM GF 10 FR natural (8744)PK GF 10 FR(40)

AKROTEK® PK-VM GF 10 FR natural (8744) is a 10% glass fibre reinforced, flame retardant and process improved Polyketone compound. The flame retardant system is free of red phosphorous, melamine, PFAS and halogenes. Due to its good chemical resistance, good dimensional stability and high elongation at break it is suitable for high voltage components in e-mobility.

Features

hydrolysis / chemically stabilised
flame retardant
process improved
E-Mobility

Properties

Modulus

4.000MPa

Strength

70MPa

Impact

48kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
4000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
70 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
48 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
8 kJ/m²

Thermal Properties


Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

0,8 mm Wall thickness
1,6 mm Wall thickness
3,2 mm Wall thickness
V-0 Class
V-0 Class
V-0 Class

GWFI

IEC 60695-2-12

0,8 mm Wall thickness
1,6 mm Wall thickness
3,2 mm Wall thickness
960 °C
960 °C
960 °C

GWIT

IEC 60695-2-13

0,8 mm Wall thickness
1,6 mm Wall thickness
825 °C
850 °C

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,34 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,5 - 0,7 %
1,1 - 1,3 %

Electrical Properties


Comparative tracking index

IEC 60112

Test liquid A
600 V

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more