AKROMID®

Preliminary

NEXT G3 GF 30 1 natural (8085)

PA6.9 GF30

AKROMID® NEXT G3 GF 30 1 natural (8085) - partly bio-based PA 6.9, low moisture absorption, increased chemical resistance.


Modulus

8.600MPa

Strength

160MPa

Impact

80kJ/m²

AKROMID® NEXT G3 GF 30 1 natural (8085) - partly bio-based PA 6.9, low moisture absorption, increased chemical resistance.

AKROMID®

B3 GF 50 4 RM-M black (3221)

PA6+X GF50

AKROMID® B3 GF 50 4 RM-M black (3221) - 50% glass fiber reinforced PA 6 with good surface properties, chemically stabilised, reduced moisture absorption


Modulus

16.500MPa

Strength

210MPa

Impact

75kJ/m²

AKROMID® B3 GF 50 4 RM-M black (3221) - 50% glass fiber reinforced PA 6 with good surface properties, chemically stabilised, reduced moisture absorption

AKROMID®

UL
Preliminary

B28 GF 25 9 FR natural (8066)

PA6 GF25 FR(40)

AKROMID® B28 GF 25 9 FR natural (8066) - PA6, 25% glass fibre, flame retardant, free of halogens, electrically neutral, heatstabilised, easy flow, UL listed V0 from 1,6 mm, e-mobility.


Modulus

8.900MPa

Strength

138MPa

Impact

83kJ/m²

AKROMID® B28 GF 25 9 FR natural (8066) - PA6, 25% glass fibre, flame retardant, free of halogens, electrically neutral, heatstabilised, easy flow, UL listed V0 from 1,6 mm, e-mobility.

AKROMID®

B3 GF 30 1 black (2485)

PA6 GF30

AKROMID® B3 GF 30 1 black (2485) - 30% glass fiber reinforced PA 6, heat stabilised, industrial engineering, automotive, also as biomass-balanced and chemical recycled PA6.


Modulus

10.300MPa

Strength

185MPa

Impact

75kJ/m²

AKROMID® B3 GF 30 1 black (2485) - 30% glass fiber reinforced PA 6, heat stabilised, industrial engineering, automotive, also as biomass-balanced and chemical recycled PA6.

AKROMID®

B3 GF 50 1 black (20008)

PA6 GF50

AKROMID® B3 GF 50 black (20008) - 50% glass fiber reinforced PA 6, heat stabilised, technical parts in industrial engineering and automotive industry


Modulus

17.000MPa

Strength

210MPa

Impact

100kJ/m²

AKROMID® B3 GF 50 black (20008) - 50% glass fiber reinforced PA 6, heat stabilised, technical parts in industrial engineering and automotive industry

AKROMID®

Preliminary

NEXT 5.10 3 GF 30 natural (8406)

PA5.10 GF30

AKROMID® NEXT 5.10 3 GF 30 natural (8406) - 100% biobased and HMD-free PA 5.10 with high strength.


Modulus

8.300MPa

Strength

160MPa

Impact

72kJ/m²

AKROMID® NEXT 5.10 3 GF 30 natural (8406) - 100% biobased and HMD-free PA 5.10 with high strength.

AKROMID®

UL
Preliminary

B28 GF 25 9 FR orange (8644)

PA6 GF25 FR(40)

AKROMID® B28 GF 25 9 FR orange (8644) - PA6, 25% glass fibre, flame retardant, free of halogens, electrically neutral, heatstabilised, easy flow, UL listed V0 from 1,6 mm, RAL 2003, e-mobility.


Modulus

9.000MPa

Strength

135MPa

Impact

81kJ/m²

AKROMID® B28 GF 25 9 FR orange (8644) - PA6, 25% glass fibre, flame retardant, free of halogens, electrically neutral, heatstabilised, easy flow, UL listed V0 from 1,6 mm, RAL 2003, e-mobility.

156780

AKROMID®

C3 5 S3 black (8029)PA66+PA6

AKROMID® C3 5 S3 black (8029) is an unreinforced, impact modified polyamide 6.6/6 blend. It is characterised by higher dry impact strength compared to standard polyamide 6.6/6 blends while maintaining good flowability. Furthermore, the material is high heat stabilised and therefore perfectly suitable for connecting and fixing systems which are used at elevated temperatures in the automotive and electro industry.

Features

heat stabilised 130
impact modified
easy flow

Properties

Modulus

2.500MPa

Strength

65MPa

Impact

180kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
2500 MPa
900 MPa

Tensile stress at yield

ISO 527-2

50 mm/min | d.a.m.
50 mm/min | conditioned
65 MPa
45 MPa

Tensile strain at break

ISO 527-2

50 mm/min | d.a.m.
50 mm/min | conditioned
> 25 %
> 250 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
2100 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
85 MPa

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
no break

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
7 kJ/m²
23 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
160 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
260 °C

Flammability


Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,12 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
1,3 - 1,5 %
1,5 - 1,7 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more