AKROTEK® PK-VM GF 40 black (8687) - Polyketon, 40% glass fibre reinforced, chemical restistant


Modulus

11.000MPa

Strength

160MPa

Impact

80kJ/m²

AKROTEK® PK-VM GF 40 black (8687) - Polyketon, 40% glass fibre reinforced, chemical restistant

AKROTEK®

Preliminary

PPS GF 30 black (8610)

PPS GF30

AKROTEK® PPS GF 30 black (8610) is a 30% glass fibre reinforced Polyphenylene sulfide with high rigidity and strength, as well as high temperature and chemical resistance.


Modulus

12.000MPa

Strength

175MPa

Impact

45kJ/m²

AKROTEK® PPS GF 30 black (8610) is a 30% glass fibre reinforced Polyphenylene sulfide with high rigidity and strength, as well as high temperature and chemical resistance.

AKROTEK®

Preliminary

PK-VM GF 40 natural (8682)

PK GF40

AKROTEK® PK-VM GF 40 natural (8682) - Polyketon, 40% glass fibre reinforced, chemical restistant


Modulus

11.000MPa

Strength

165MPa

Impact

78kJ/m²

AKROTEK® PK-VM GF 40 natural (8682) - Polyketon, 40% glass fibre reinforced, chemical restistant

AKROTEK®

Preliminary

AM ICF 20 black (8722)

ABSCF20

AKROTEK® AM ICF 20 black (8722) - recycled carbon fibre reinforced for additive manufacturing (3D-printing)


Modulus

13.400MPa

Strength

100MPa

Impact

20kJ/m²

AKROTEK® AM ICF 20 black (8722) - recycled carbon fibre reinforced for additive manufacturing (3D-printing)

AKROMID®

A3 GF 50 4 natural (71090)

PA66 GF50

AKROMID® A3 GF 50 4 natural (71090) - PA6.6, 50% glass fiber, cooling water, hydrolysis resistant, DPPD free


Modulus

18.000MPa

Strength

260MPa

Impact

110kJ/m²

AKROMID® A3 GF 50 4 natural (71090) - PA6.6, 50% glass fiber, cooling water, hydrolysis resistant, DPPD free

AKROMID®

Preliminary

NEXT G3 GF 30 1 black (8468)

PA6.9 GF30

AKROMID® NEXT G3 GF 30 1 black (8468) - PA 6.9, 30% glass fibre, low moisture absorption, increased chemical resistance, good strength, good stiffness, industrial.


Modulus

8.600MPa

Strength

160MPa

Impact

80kJ/m²

AKROMID® NEXT G3 GF 30 1 black (8468) - PA 6.9, 30% glass fibre, low moisture absorption, increased chemical resistance, good strength, good stiffness, industrial.

AKROMID®

Preliminary

C3 GF 30 8 black (5657)

PA66 + PA6 GF30

AKROMID® C3 GF 30 8 black (5657) - PA6.6/6 Blend, GF 30, FDA, EU 10/2010, food contact, kitchen and household appliances


Modulus

9.400MPa

Strength

190MPa

Impact

82kJ/m²

AKROMID® C3 GF 30 8 black (5657) - PA6.6/6 Blend, GF 30, FDA, EU 10/2010, food contact, kitchen and household appliances

175767780

AKROMID®

B3 GF 45 1 black (3851)PA6 GF45

AKROMID® B3 GF 45 1 black (3851) is a 45% glass fibre reinforced, heat stabilised polyamide 6 with very high rigidity and strength

Features

heat stabilised 130

Properties

Modulus

14.500MPa

Strength

200MPa

Impact

110kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
14500 MPa
8500 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
200 MPa
140 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
4,5 %
8,5 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
13000 MPa
7500 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
315 MPa
200 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
4,5 %
6,7 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
30°C | conditioned
-
110 kJ/m²
108 kJ/m²
95 kJ/m²
108 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
30°C | conditioned
-
20 kJ/m²
25 kJ/m²
16 kJ/m²
15 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
200 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
220 °C

Temperature of deflection under load HDT/C

ISO 75

8 MPa
145 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,5 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,3 %
0,8 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more