AKROMID®

A3 GFM 25/15 1 black (3335)

PA66 (GF25+MD15)

AKROMID® A3 GFM 25/15 1 black (3335) is a 25% glass fibre reinforced, 15% mineral filled, heat stabilised polyamide 6.6 with good surface and dimensional stability


Modulus

10.000MPa

Strength

150MPa

Impact

50kJ/m²

AKROMID® A3 GFM 25/15 1 black (3335) is a 25% glass fibre reinforced, 15% mineral filled, heat stabilised polyamide 6.6 with good surface and dimensional stability

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)

PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.


Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

AKROMID®

Preliminary

A3 black (7557)

PA66

AKROMID® A3 black (7557) is an unreinforced, UV stabilised polyamide 6.6.


Modulus

3.200MPa

Strength

80MPa

Impact

180kJ/m²

AKROMID® A3 black (7557) is an unreinforced, UV stabilised polyamide 6.6.

AKROMID®

Preliminary

B+ GF 30 6 LT black (7665)

PA6 GF30

High-heat stabilised, laser transparent PA6 compound with enhanced mechanical properties in conditioned state to substitute PA 66 compounds


Modulus

10.000MPa

Strength

185MPa

Impact

95kJ/m²

High-heat stabilised, laser transparent PA6 compound with enhanced mechanical properties in conditioned state to substitute PA 66 compounds

AKROMID®

UL

C3 GF 30 1 FR orange (7855)

PA6+PA66 GF30 FR(40)

AKROMID® C3 GF 30 1 FR orange (7855) - PA6/6.6 blend, 30 % glass fiber, flame retardant, good flowability, UL-listed, RAL 2003, E&E, Public transportation EN 45545-2.


Modulus

10.600MPa

Strength

135MPa

Impact

65kJ/m²

AKROMID® C3 GF 30 1 FR orange (7855) - PA6/6.6 blend, 30 % glass fiber, flame retardant, good flowability, UL-listed, RAL 2003, E&E, Public transportation EN 45545-2.

AKROLOY®

PA GF 50 white (5137)

PA66+PA6I/6T GF50

AKROLOY® PA GF 50 white (5137) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.


Modulus

20.000MPa

Strength

250MPa

Impact

105kJ/m²

AKROLOY® PA GF 50 white (5137) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.

AKROMID®

Preliminary

B3 1 S3 natural (8013)

PA6-I

AKROMID® B3 1 S3 natural (8013) - PA 6 unreinforced, impact modified, connecting and fixing systems.


Modulus

2.200MPa

Strength

55MPa

Impact

180kJ/m²

AKROMID® B3 1 S3 natural (8013) - PA 6 unreinforced, impact modified, connecting and fixing systems.

171727380

AKROMID®

D3 GF 30 2 black (7026)PA612 GF30

AKROMID® D3 GF 30 2 black (7026) is a 30% glass fibre reinforced, UV-stabilised polyamide 6.12 with high strength and stiffness. Due to its good chemical resistance, the compound is suitable for media-carrying connectors, which are exposed to UV radiation.

Features

UV-stabilised
reduced moisture

Properties

Modulus

9.500MPa

Strength

180MPa

Impact

95kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
9500 MPa
7000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
180 MPa
120 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
3,5 %
4,4 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
95 kJ/m²
80 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
15 kJ/m²
15 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
200 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
215 °C

Flammability


Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,31 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
1,4 %

Molding shrinkage

ISO 294-4

flow
transverse
0,4 %
0,9 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more