AKROMID®

Preliminary

T5 GF 40 6 black (8002)

PPA GF40

AKROMID® T5 GF 40 6 black (8002) - 40% glass fibre reinforced with high stiffness and strength, high temperature resistance, e.g. under the hood applications


Modulus

16.000MPa

Strength

245MPa

Impact

80kJ/m²

AKROMID® T5 GF 40 6 black (8002) - 40% glass fibre reinforced with high stiffness and strength, high temperature resistance, e.g. under the hood applications

AKROMID®

C3 1 S3 black (4297)

PA66+PA6

AKROMID® C3 1 S3 black (4297) - PA 6.6/6 blend unreinforced, impact modified whilst maintaining good flowability, for connecting and fixing systems


Modulus

2.500MPa

Strength

65MPa

Impact

180kJ/m²

AKROMID® C3 1 S3 black (4297) - PA 6.6/6 blend unreinforced, impact modified whilst maintaining good flowability, for connecting and fixing systems

AKROMID®

Preliminary

B3 GM 10/20 1 black (8748)

PA6 (GF10+GB20)

AKROMID® B3 GM 10/20 1 black (8748) - PA6, 10% glass fibre, 20% glass bead, heat stabilised, easy flowing, good surface, reduced warpage.


Modulus

5.700MPa

Strength

110MPa

Impact

30kJ/m²

AKROMID® B3 GM 10/20 1 black (8748) - PA6, 10% glass fibre, 20% glass bead, heat stabilised, easy flowing, good surface, reduced warpage.

AKROMID®

A3 2 S1 white (5973)

PA66-I

AKROMID® A3 2 S1 white (5973) - PA 6.6, unreinforced, impact modified, UV-stabilised, for connecting and fixing systems, automotive, electro, furniture


Modulus

1.700MPa

Strength

45MPa

Impact

180kJ/m²

AKROMID® A3 2 S1 white (5973) - PA 6.6, unreinforced, impact modified, UV-stabilised, for connecting and fixing systems, automotive, electro, furniture

AKROTEK®

PK-VM 8 natural (6146)

PK

AKROTEK® PK-VM 8 natural (6146) - Polyketon, unreinforced, Tribology, friction and wear, chemical resistance, EU 10/2011, FDA 21 CFR


Modulus

1.500MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-VM 8 natural (6146) - Polyketon, unreinforced, Tribology, friction and wear, chemical resistance, EU 10/2011, FDA 21 CFR

AKROMID®

B3 GF 15 grey (6270)

PA6 GF15

AKROMID® B3 GF 15 grey (6270) is a 15% glass fibre reinforced polyamide 6 with average stiffness and strength.


Modulus

6.000MPa

Strength

110MPa

Impact

50kJ/m²

AKROMID® B3 GF 15 grey (6270) is a 15% glass fibre reinforced polyamide 6 with average stiffness and strength.

AKROMID®

UL

A3 GF 30 HU grey (6600)

PA66 GF30

AKROMID® A3 GF 30 HU grey (6600) is a 30% glass fibre reinforced, heat stabilised polyamide 6.6 with high rigidity and strength, listet at UL in all colors


Modulus

10.500MPa

Strength

200MPa

Impact

85kJ/m²

AKROMID® A3 GF 30 HU grey (6600) is a 30% glass fibre reinforced, heat stabilised polyamide 6.6 with high rigidity and strength, listet at UL in all colors

149505180

AKROLEN®

Internal

PP LGF 40 2 black (6911)PP LGF40

AKROLEN® PP LGF 40 2 black (6911) is a polypropylene homopolymer with 40% long glass fibre reinforcement which leads to a very high stiffness and strength. The materials very good surface quality as well as the outstanding UV-stability make it the product of your choice for technical parts which are exposed to UV radiation.

Features

UV-stabilised

Properties

Modulus

10.000MPa

Strength

140MPa

Impact

75kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
10000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
140 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
2 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
10000 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
200 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
2,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
30°C | d.a.m.
-
75 kJ/m²
70 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
30°C | d.a.m.
-
30 kJ/m²
32 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
165 °C

Temperature of deflection under load HDT/C

ISO 75

8 MPa
145 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
165 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,22 g/cm³

Electrical Properties


Volume resistivity IEC

DIN EN IEC 62631-3-2

d.a.m.
1012 Ω x cm

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more