AKROLOY®

PA GF 50 natural (6414)

PA66+PA6I/6T GF50

AKROLOY® PA GF 50 natural (6414) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.


Modulus

17.000MPa

Strength

275MPa

Impact

110kJ/m²

AKROLOY® PA GF 50 natural (6414) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.

AKROMID®

T5 GF 35 4 black (7692)

PPA GF35

AKROMID® T5 GF 35 4 black (7692) is a 35% glass fibre reinforced polyphthalamide with inorganic heat stabilization, very high rigidity and strength, designed for hydrolysis resistance. This aromatic PPA keeps mechanical performance even at elevated temperatures or moisture pic-up


Modulus

13.500MPa

Strength

220MPa

Impact

70kJ/m²

AKROMID® T5 GF 35 4 black (7692) is a 35% glass fibre reinforced polyphthalamide with inorganic heat stabilization, very high rigidity and strength, designed for hydrolysis resistance. This aromatic PPA keeps mechanical performance even at elevated temperatures or moisture pic-up

AKROMID®

Preliminary

T9 GF 50 black (7601)

PPA GF50

AKROMID® T9 GF 50 black (7601) is a 50% glass fibre reinforced partially aromatic polyphthalamide with very high stiffness and strength, as well as high temperature and chemical resistance. The compound is based on PA9T and has lower moisture uptake than conventional PA6T variants. This leads to a significantly higher consistency of the glass transition temperature and higher strength at elevated temperatures especially in conditioned state.


Modulus

17.000MPa

Strength

250MPa

Impact

95kJ/m²

AKROMID® T9 GF 50 black (7601) is a 50% glass fibre reinforced partially aromatic polyphthalamide with very high stiffness and strength, as well as high temperature and chemical resistance. The compound is based on PA9T and has lower moisture uptake than conventional PA6T variants. This leads to a significantly higher consistency of the glass transition temperature and higher strength at elevated temperatures especially in conditioned state.

AKROMID®

A3 GM 20/10 4 WIT black (4529)

PA66 (GF20+GB10)

AKROMID® A3 GM 20/10 4 WIT black (4529) - 20% glass fibre, 10% glass bead, hydrolysis/chemical, polyamide 6.6, good surface, low warpage


Modulus

8.200MPa

Strength

175MPa

Impact

65kJ/m²

AKROMID® A3 GM 20/10 4 WIT black (4529) - 20% glass fibre, 10% glass bead, hydrolysis/chemical, polyamide 6.6, good surface, low warpage

AKROMID®

D3 GF 30 1 black (5392)

PA612 GF30

AKROMID® D3 GF 30 1 black (5392) - PA 6.12, 30% glass fiber, connector


Modulus

9.500MPa

Strength

180MPa

Impact

95kJ/m²

AKROMID® D3 GF 30 1 black (5392) - PA 6.12, 30% glass fiber, connector

AKROMID®

A28 LGF 50 9 black (7705)

PA66 LGF50

AKROMID® A28 LGF 50 9 black (7705) - 50% long glass fiber reinforced PA6.6, easy flowing, process improved, low shrinkage, very good fatigue performance, oil pan


Modulus

18.000MPa

Strength

270MPa

Impact

95kJ/m²

AKROMID® A28 LGF 50 9 black (7705) - 50% long glass fiber reinforced PA6.6, easy flowing, process improved, low shrinkage, very good fatigue performance, oil pan

AKROTEK®

PK-VM natural (4774)

PK

AKROTEK® PK-VM natural (4774) - Polyketon, Tribology, friction and wear, chemical resistance


Modulus

1.500MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-VM natural (4774) - Polyketon, Tribology, friction and wear, chemical resistance

1891080

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

Features

hydrolysis / chemically stabilised

Properties

Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
5800 MPa
5600 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
100 MPa
90 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
2,5 %
2,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
50 kJ/m²
45 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
210 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,4 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
0,6 - 0,7 %

Molding shrinkage

ISO 294-4

flow
transverse
0,4 - 0,6 %
0,9 - 1,1 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more