AKROTEK®

Preliminary

PPS GF 40 black (8609)

PPS GF40

AKROTEK® PPS GF 40 black (8609) is a 40% glass fibre reinforced Polyphenylene sulfide with high rigidity and strength, as well as high temperature and chemical resistance.


Modulus

16.000MPa

Strength

180MPa

Impact

50kJ/m²

AKROTEK® PPS GF 40 black (8609) is a 40% glass fibre reinforced Polyphenylene sulfide with high rigidity and strength, as well as high temperature and chemical resistance.

AKROTEK®

Preliminary

PK-VM GF 10 natural (8679)

PK GF10

AKROTEK® PK-VM GF 10 natural (8679) - Polyketon, 10% glass fibre reinforced, chemical and hydrolysis resistance


Modulus

3.600MPa

Strength

75MPa

Impact

61kJ/m²

AKROTEK® PK-VM GF 10 natural (8679) - Polyketon, 10% glass fibre reinforced, chemical and hydrolysis resistance

AKROMID®

Preliminary

C3 GF 30 8 black (5657)

PA66 + PA6 GF30

AKROMID® C3 GF 30 8 black (5657) - PA6.6/6 Blend, GF 30, FDA, EU 10/2010, food contact, kitchen and household appliances


Modulus

9.400MPa

Strength

190MPa

Impact

82kJ/m²

AKROMID® C3 GF 30 8 black (5657) - PA6.6/6 Blend, GF 30, FDA, EU 10/2010, food contact, kitchen and household appliances

AKROTEK®

Preliminary

PK-VM GF 40 natural (8682)

PK GF40

AKROTEK® PK-VM GF 40 natural (8682) - Polyketon, 40% glass fibre reinforced, chemical restistant


Modulus

11.000MPa

Strength

165MPa

Impact

78kJ/m²

AKROTEK® PK-VM GF 40 natural (8682) - Polyketon, 40% glass fibre reinforced, chemical restistant

AKROTEK®

Preliminary

PK-VM GF 60 natural (8684)

PK GF60

AKROTEK® PK-VM GF 60 natural (8684) - Polyketon, 60% glass fibre reinforced, chemical and hydrolysis resistance


Modulus

17.500MPa

Strength

180MPa

Impact

70kJ/m²

AKROTEK® PK-VM GF 60 natural (8684) - Polyketon, 60% glass fibre reinforced, chemical and hydrolysis resistance

AKROMID®

A3 S3 natural (1176)

PA66-I

AKROMID® A3 S3 natural (1176) - PA 6.6, unreinforced, dry impact modified, for connecting and fixing systems, automotive, E&E


Modulus

2.800MPa

Strength

67MPa

Impact

180kJ/m²

AKROMID® A3 S3 natural (1176) - PA 6.6, unreinforced, dry impact modified, for connecting and fixing systems, automotive, E&E

AKROMID®

Preliminary

T5 GF 20 8 black (6456)

PPA GF20

AKROMID® T5 GF 20 8 black (6456) - PPA, 20% glass fiber, food contact, kitchen and household appliances, fitting, water meter, ACS, WRAS, NSF 61, EU 10/2011, FDA


Modulus

8.500MPa

Strength

160MPa

Impact

40kJ/m²

AKROMID® T5 GF 20 8 black (6456) - PPA, 20% glass fiber, food contact, kitchen and household appliances, fitting, water meter, ACS, WRAS, NSF 61, EU 10/2011, FDA

176777880

AKROMID®

B3 ICF 40 black (5020)PA6 CF40

AKROMID® B3 ICF 40 black (5020) is a 40% carbon fibre reinforced polyamide 6 with high flexural strength and good sliding properties

Properties

Modulus

30.000MPa

Strength

220MPa

Impact

60kJ/m²

Sustainability


Recycled content

40 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
30000 MPa
14000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
220 MPa
135 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
1,7 %
3 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
25000 MPa
17000 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
320 MPa
215 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
1,8 %
2,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
60 kJ/m²
65 kJ/m²
50 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
10 kJ/m²
15 kJ/m²
8 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
210 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Coefficient of linear thermal expansion

ISO 11359-1/2

23°C to 80°C | parallel
23°C to 80°C | transverse
0,17 10⁻⁴/K
0,73 10⁻⁴/K

Thermal conductivity

DIN 52612

0,41 W/mK

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,31 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
1,8 - 2,0 %

Molding shrinkage

ISO 294-4

flow
transverse
0,1 - 0,3 %
0,4 - 0,6 %

Electrical Properties


Surface resistivity

DIN EN 62631-3-2

d.a.m.
conditioned
103
103

Rheological Properties


Flowability

AKRO

2 mm Thickness
300 mm

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more