AKROTEK®

Preliminary

PK-VM GF 15 8 black (6991)

PK GF15

AKROTEK® PK-VM GF 15 8 black (6991) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

4.500MPa

Strength

95MPa

Impact

55kJ/m²

AKROTEK® PK-VM GF 15 8 black (6991) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

PRECITE®

Preliminary

E GF 20 natural (7301)

PET GF 20

PRECITE® E GF 20 natural (7301) - PET, 20% glass fibre, good stiffness, good toughness, elevated temperature, good surface, dimensional stability, metal replacement, automotive, E&E, household.


Modulus

7.800MPa

Strength

145MPa

Impact

40kJ/m²

PRECITE® E GF 20 natural (7301) - PET, 20% glass fibre, good stiffness, good toughness, elevated temperature, good surface, dimensional stability, metal replacement, automotive, E&E, household.

AKROLEN®

Preliminary

PP ICF 30 AM black (8344)

PP CF30

AKROLEN® PP ICF 30 AM black (8344) - recycled carbon fibre reinforced polypropylene for additive manufacturing (3D-printing)


Modulus

12.500MPa

Strength

85MPa

Impact

50kJ/m²

AKROLEN® PP ICF 30 AM black (8344) - recycled carbon fibre reinforced polypropylene for additive manufacturing (3D-printing)

AKROMID®

A3 GF 50 4 natural (71090)

PA66 GF50

AKROMID® A3 GF 50 4 natural (71090) - PA6.6, 50% glass fiber, cooling water, hydrolysis resistant, DPPD free


Modulus

18.000MPa

Strength

260MPa

Impact

110kJ/m²

AKROMID® A3 GF 50 4 natural (71090) - PA6.6, 50% glass fiber, cooling water, hydrolysis resistant, DPPD free

AKROMID®

B3 GF 30 1 grey (7574)

PA6 GF30

AKROMID® B3 GF 30 1 grey (7574) is a 30% glass fibre reinforced, heat stabilised polyamide 6 with high rigidity and strength


Modulus

9.900MPa

Strength

168MPa

Impact

NA

AKROMID® B3 GF 30 1 grey (7574) is a 30% glass fibre reinforced, heat stabilised polyamide 6 with high rigidity and strength

AKROTEK®

Preliminary

PPS GF 30 black (8610)

PPS GF30

AKROTEK® PPS GF 30 black (8610) is a 30% glass fibre reinforced Polyphenylene sulfide with high rigidity and strength, as well as high temperature and chemical resistance.


Modulus

12.000MPa

Strength

175MPa

Impact

45kJ/m²

AKROTEK® PPS GF 30 black (8610) is a 30% glass fibre reinforced Polyphenylene sulfide with high rigidity and strength, as well as high temperature and chemical resistance.

AKROTEK®

Preliminary

PK-VM GF 15 natural (8680)

PK GF15

AKROTEK® PK-VM GF 15 natural (8680) - Polyketon, 15% glass fiber reinforced, chemical and hydrolysis resistance


Modulus

4.600MPa

Strength

100MPa

Impact

65kJ/m²

AKROTEK® PK-VM GF 15 natural (8680) - Polyketon, 15% glass fiber reinforced, chemical and hydrolysis resistance

174757680

AKROLOY®

PA GF 50 grey (3807)PA66 + PA6I/6T GF50

AKROLOY® PA GF 50 grey (3807) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength.

Properties

Modulus

17.200MPa

Strength

250MPa

Impact

105kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
17200 MPa
16500 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
250 MPa
220 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
2,7 %
3 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
13200 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
360 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
3,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
105 kJ/m²
100 kJ/m²
95 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
16 kJ/m²
17 kJ/m²
15 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
221 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
245 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
255 °C

Flammability


Burning rate

UL 94

0,8 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,59 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,2 %
0,6 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.