HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROMID®

C3 GF 60 1 black (4659)

PA66 + PA6 GF60

AKROMID® C3 GF 60 1 black (4659) is a 60% glass fibre reinforced, heat stabilised polyamide 6.6/6 - Blend.


Modulus

21.300MPa

Strength

270MPa

Impact

96kJ/m²

AKROMID® C3 GF 60 1 black (4659) is a 60% glass fibre reinforced, heat stabilised polyamide 6.6/6 - Blend.

AKROMID®

A3 GF 40 1 L black (4671)

PA66+PP GF40

AKROMID® A3 GF 40 1 L black (4671) - PA6.6/PP-Blend, 40% glass fibre reinforced, lower density, cost reduced, zinc chloride


Modulus

11.800MPa

Strength

170MPa

Impact

80kJ/m²

AKROMID® A3 GF 40 1 L black (4671) - PA6.6/PP-Blend, 40% glass fibre reinforced, lower density, cost reduced, zinc chloride

AKROMID®

Preliminary

B28 GF 15 natural (6940)

PA6 GF 15

AKROMID B28 GF 15 natural (6940) - PA 6, glass fiber reinforced, easy flow, good surface, bus fire standard ECE R 118.03, medium stiffness and strength.


Modulus

5.300MPa

Strength

120MPa

Impact

39kJ/m²

AKROMID B28 GF 15 natural (6940) - PA 6, glass fiber reinforced, easy flow, good surface, bus fire standard ECE R 118.03, medium stiffness and strength.

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)

PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.


Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

AKROTEK®

Preliminary

PK-VM GF 40 8 black (6995)

PK GF40

AKROTEK® PK-VM GF 40 8 black (6995) - Polyketon, 40% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

11.000MPa

Strength

150MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 40 8 black (6995) - Polyketon, 40% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

PRECITE®

Preliminary

E GF 20 natural (7301)

PET GF 20

PRECITE® E GF 20 natural (7301) - PET, 20% glass fibre, good stiffness, good toughness, elevated temperature, good surface, dimensional stability, metal replacement, automotive, E&E, household.


Modulus

7.800MPa

Strength

145MPa

Impact

40kJ/m²

PRECITE® E GF 20 natural (7301) - PET, 20% glass fibre, good stiffness, good toughness, elevated temperature, good surface, dimensional stability, metal replacement, automotive, E&E, household.

AKROMID®

A3 5 black (4701)

PA66

AKROMID® A3 5 black (4701) is an unreinforced, high temperature stabilised polyamide 6.6


Modulus

3.500MPa

Strength

90MPa

Impact

180kJ/m²

AKROMID® A3 5 black (4701) is an unreinforced, high temperature stabilised polyamide 6.6

173747580

AKROMID®

S3 GF 15 5 black (6062)PA610 GF15

AKROMID® S3 GF 15 5 black (6062) is a 15% glass fibre reinforced, high temperature stabilised polyamide 6.10 with average stiffness and strength and lower moisture absorption and high chemical resistance.

Properties

Modulus

5.500MPa

Strength

120MPa

Impact

65kJ/m²

Sustainability


Biobased carbon content

59 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
5500 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
120 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
4 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
4800 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
180 MPa

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
65 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
6 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
200 °C

Temperature of deflection under load HDT/C

ISO 75

8 MPa
75 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

0,8 mm Wall thickness
1,6 mm Wall thickness
HB Class
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,18 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
1,4 - 1,6 %

Molding shrinkage

ISO 294-4

flow
transverse
0,4 - 0,6 %
0,9 - 1,1 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more