AKROMID®

B3 black (2502)

PA6

AKROMID® B3 black (2502) is an unreinforced polyamide 6.


Modulus

3.600MPa

Strength

85MPa

Impact

180kJ/m²

AKROMID® B3 black (2502) is an unreinforced polyamide 6.

AKROMID®

B3 1 natural (2499)

PA6

AKROMID® B3 1 natural (2499) is an unreinforced, heat stabilised polyamide 6 with light inherent color


Modulus

3.600MPa

Strength

85MPa

Impact

180kJ/m²

AKROMID® B3 1 natural (2499) is an unreinforced, heat stabilised polyamide 6 with light inherent color

AKROMID®

B3 ICF 40 black (5020)

PA6 CF40

AKROMID® B3 ICF 40 black (5020) is a 40% carbon fibre reinforced polyamide 6 with high flexural strength and good sliding properties


Modulus

30.000MPa

Strength

220MPa

Impact

60kJ/m²

AKROMID® B3 ICF 40 black (5020) is a 40% carbon fibre reinforced polyamide 6 with high flexural strength and good sliding properties

AKROTEK®

PK-VM GF 50 8 black (6936)

PK GF50

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

14.000MPa

Strength

170MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)

PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.


Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

AKROMID®

Preliminary

B3 1 S3 natural (8013)

PA6-I

AKROMID® B3 1 S3 natural (8013) - PA 6 unreinforced, impact modified, connecting and fixing systems.


Modulus

2.200MPa

Strength

55MPa

Impact

180kJ/m²

AKROMID® B3 1 S3 natural (8013) - PA 6 unreinforced, impact modified, connecting and fixing systems.

AKROLOY®

PA GF 60 black (7789)

PA66+PA6I/6T GF60

AKROLOY® PA GF 60 black (7789) is a 60% glass fibre reinforced, easyflow, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.


Modulus

21.400MPa

Strength

290MPa

Impact

100kJ/m²

AKROLOY® PA GF 60 black (7789) is a 60% glass fibre reinforced, easyflow, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.

168697080

AKROMID®

Preliminary

B3 GM 10/20 1 black (8748)PA6 (GF10+GB20)

AKROMID® B3 GM 10/20 1 black (8748) is a 10% glass fiber and 20% glass beads reinforced easy flowing PA 6. It is characterised by a medium stiffness and strength. The material impresses with very good surface properties and is therefore perfectly suitable for housings and covers in the automotive industry with high demands on the surface.

Features

heat stabilised 130
recycled content
easy flow

Properties

Modulus

5.700MPa

Strength

110MPa

Impact

30kJ/m²

Sustainability


Recycled content

20 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
5700 MPa
3000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
110 MPa
60 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
2,6 %
10 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
30 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
4 kJ/m²
7 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
200 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

GWFI

IEC 60695-2-12

1,6 mm Wall thickness
650 °C

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,35 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
2,2 %

Molding shrinkage

ISO 294-4

flow
transverse
0,3 - 0,5 %
0,6 - 0,8 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more