HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROMID®

B3 black (2502)

PA6

AKROMID® B3 black (2502) is an unreinforced polyamide 6.


Modulus

3.600MPa

Strength

85MPa

Impact

180kJ/m²

AKROMID® B3 black (2502) is an unreinforced polyamide 6.

AKROMID®

B3 1 natural (2499)

PA6

AKROMID® B3 1 natural (2499) is an unreinforced, heat stabilised polyamide 6 with light inherent color


Modulus

3.600MPa

Strength

85MPa

Impact

180kJ/m²

AKROMID® B3 1 natural (2499) is an unreinforced, heat stabilised polyamide 6 with light inherent color

AKROMID®

B3 ICF 40 black (5020)

PA6 CF40

AKROMID® B3 ICF 40 black (5020) is a 40% carbon fibre reinforced polyamide 6 with high flexural strength and good sliding properties


Modulus

30.000MPa

Strength

220MPa

Impact

60kJ/m²

AKROMID® B3 ICF 40 black (5020) is a 40% carbon fibre reinforced polyamide 6 with high flexural strength and good sliding properties

AKROTEK®

PK-VM GF 50 8 black (6936)

PK GF50

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

14.000MPa

Strength

170MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)

PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.


Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

AKROMID®

Preliminary

B3 1 S3 natural (8013)

PA6-I

AKROMID® B3 1 S3 natural (8013) - PA 6 unreinforced, impact modified, connecting and fixing systems.


Modulus

2.200MPa

Strength

55MPa

Impact

180kJ/m²

AKROMID® B3 1 S3 natural (8013) - PA 6 unreinforced, impact modified, connecting and fixing systems.

AKROLOY®

PA GF 60 black (7789)

PA66+PA6I/6T GF60

AKROLOY® PA GF 60 black (7789) is a 60% glass fibre reinforced, easyflow, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.


Modulus

21.400MPa

Strength

290MPa

Impact

100kJ/m²

AKROLOY® PA GF 60 black (7789) is a 60% glass fibre reinforced, easyflow, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.

168697080

AKROMID®

B3 GM 10/20 1 L black (4646)PA6+PP (GF10+GB20)

AKROMID® B3 GM 10/20 1 L black (4646) is a PA6/PP-blend with reduced density compared to standard PA6 GM 10/20. With 10% glass fibre reinforcement and 20% glass bead filling the material is suitable for components with average strength and stiffness where cost and weight reduction are required at the same time. The chemical resistance of AKROMID® B3 GM 10/20 1 L black (4646) is particularly superior to calcium chloride (CaCl₂).

Features

heat stabilised 130
reduced density

Properties

Modulus

5.100MPa

Strength

88MPa

Impact

46kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
5100 MPa
3300 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
88 MPa
55 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
3,4 %
6 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
4700 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
130 MPa

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
30°C | conditioned
-
46 kJ/m²
44 kJ/m²
43 kJ/m²
42 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
30°C | conditioned
-
7 kJ/m²
9 kJ/m²
4 kJ/m²
4 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
165 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
208 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

0,8 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,26 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
1,4 %

Molding shrinkage

ISO 294-4

flow
transverse
0,3 - 0,5 %
0,6 - 0,8 %

Rheological Properties


MVR

ISO 1133

275°C/5kg
18 cm³/10 min

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more