AKROMID®

A3 GF 25 3 black (3094)

PA66 GF25

AKROMID® A3 GF 25 3 black (3094) is a 25% glass fibre reinforced, nucleated polyamide 6.6 with high stiffness and strength


Modulus

8.500MPa

Strength

160MPa

Impact

50kJ/m²

AKROMID® A3 GF 25 3 black (3094) is a 25% glass fibre reinforced, nucleated polyamide 6.6 with high stiffness and strength

AKROMID®

Preliminary

S3 GF 30 4 black (3429)

PA610 GF30

AKROMID® S3 GF 30 4 black (3429) is a 30% glass fibre reinforced and hydrolysis stabilised polyamide 6.10 with high stiffness and strength as well as lower moisture absorption and very high chemical resistance.


Modulus

8.600MPa

Strength

160MPa

Impact

110kJ/m²

AKROMID® S3 GF 30 4 black (3429) is a 30% glass fibre reinforced and hydrolysis stabilised polyamide 6.10 with high stiffness and strength as well as lower moisture absorption and very high chemical resistance.

AKROTEK®

PK-VM ICF 15 black (6074)

PK CF15

AKROTEK® PK-VM ICF 15 black (6074) is a 15% carbon fibre reinforced polyketon with good sliding properties.


Modulus

9.000MPa

Strength

90MPa

Impact

30kJ/m²

AKROTEK® PK-VM ICF 15 black (6074) is a 15% carbon fibre reinforced polyketon with good sliding properties.

AKROMID®

A3 GK 30 6 natural (6774)

PA66 GB30

AKROMID® A3 GK 30 6 natural (6774) - 30% glass bead, inorganic high temperature stabilised, polyamide 6.6, low warpage, high surface appearance


Modulus

4.600MPa

Strength

90MPa

Impact

25kJ/m²

AKROMID® A3 GK 30 6 natural (6774) - 30% glass bead, inorganic high temperature stabilised, polyamide 6.6, low warpage, high surface appearance

AKROTEK®

PK-VM GF 50 8 black (6936)

PK GF50

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

14.000MPa

Strength

170MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROTEK®

PK-VM GF 30 8 natural (6983)

PK GF30

AKROTEK® PK-VM GF 30 8 natural (6983) - Polyketon, 30% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

8.200MPa

Strength

130MPa

Impact

60kJ/m²

AKROTEK® PK-VM GF 30 8 natural (6983) - Polyketon, 30% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROMID®

Preliminary

B+ GF 30 6 LT black (7665)

PA6 GF30

High-heat stabilised, laser transparent PA6 compound with enhanced mechanical properties in conditioned state to substitute PA 66 compounds


Modulus

10.000MPa

Strength

185MPa

Impact

95kJ/m²

High-heat stabilised, laser transparent PA6 compound with enhanced mechanical properties in conditioned state to substitute PA 66 compounds

165666780

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

Features

hydrolysis / chemically stabilised

Properties

Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
5800 MPa
5600 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
100 MPa
90 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
2,5 %
2,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
50 kJ/m²
45 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
210 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,4 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
0,6 - 0,7 %

Molding shrinkage

ISO 294-4

flow
transverse
0,4 - 0,6 %
0,9 - 1,1 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more