B3 ICF 40 black (5020)

PA6 CF40

AKROMID® B3 ICF 40 black (5020) is a 40% carbon fibre reinforced polyamide 6 with high flexural strength and good sliding properties


Modulus

30.000MPa

Strength

220MPa

Impact

60kJ/m²

AKROMID® B3 ICF 40 black (5020) is a 40% carbon fibre reinforced polyamide 6 with high flexural strength and good sliding properties

AKROMID®

A3 GK 30 6 natural (6774)

PA66 GB30

AKROMID® A3 GK 30 6 natural (6774) - 30% glass bead, inorganic high temperature stabilised, polyamide 6.6, low warpage, high surface appearance


Modulus

4.600MPa

Strength

90MPa

Impact

25kJ/m²

AKROMID® A3 GK 30 6 natural (6774) - 30% glass bead, inorganic high temperature stabilised, polyamide 6.6, low warpage, high surface appearance

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)

PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.


Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

AKROMID®

A3 GF 50 4 black (7282)

PA66 GF50

AKROMID® A3 GF 50 4 black (7282) is a 50% glass fibre reinforced, hydrolysis/chemical stabilised polyamide 6.6 with very high rigidity and strength


Modulus

17.000MPa

Strength

250MPa

Impact

110kJ/m²

AKROMID® A3 GF 50 4 black (7282) is a 50% glass fibre reinforced, hydrolysis/chemical stabilised polyamide 6.6 with very high rigidity and strength

AKROMID®

B3 GF 25 natural (2471)

PA6 GF25

AKROMID® B3 GF 25 natural (2471) is a 25% glass fibre reinforced polyamide 6 with high stiffness and strength and light inherent color


Modulus

8.500MPa

Strength

160MPa

Impact

85kJ/m²

AKROMID® B3 GF 25 natural (2471) is a 25% glass fibre reinforced polyamide 6 with high stiffness and strength and light inherent color

AKROMID®

B3 1 natural (2499)

PA6

AKROMID® B3 1 natural (2499) is an unreinforced, heat stabilised polyamide 6 with light inherent color


Modulus

3.600MPa

Strength

85MPa

Impact

180kJ/m²

AKROMID® B3 1 natural (2499) is an unreinforced, heat stabilised polyamide 6 with light inherent color

AKROMID®

A3 GF 25 3 black (3094)

PA66 GF25

AKROMID® A3 GF 25 3 black (3094) is a 25% glass fibre reinforced, nucleated polyamide 6.6 with high stiffness and strength


Modulus

8.500MPa

Strength

160MPa

Impact

50kJ/m²

AKROMID® A3 GF 25 3 black (3094) is a 25% glass fibre reinforced, nucleated polyamide 6.6 with high stiffness and strength

165666780

AKROMID®

A3 GF 13 S3 black (3768)PA66-I GF13

AKROMID® A3 GF 13 S3 black (3768) is a 13% glass fiber reinforced, impact modified PA 6.6. It is characterised by a higher impact strength compared to standard glass fiber reinforced PA 6.6 and therefore perfectly suitable for technical applications in the mechanical engineering and automotive industry.

Features

impact modified

Properties

Modulus

5.200MPa

Strength

125MPa

Impact

75kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
5200 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
125 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
4 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
4800 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
180 MPa

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
30°C | d.a.m.
-
75 kJ/m²
55 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
30°C | d.a.m.
-
11 kJ/m²
6 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
244 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
261 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
260 °C

General properties


Density

ISO 1183

23°C
1,2 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,3 %
0,9 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more