HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROLOY®

PA GF 40 black (2845)

PA66 + PA6I/6T GF40

AKROLOY® PA GF 40 black (2845) is a 40% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state. The advanced version of this Product is AKROLOY® PA GF 40 black (6416) with a modern stabilization technology, featuring improved weld-line strength and an even wider process window.


Modulus

13.000MPa

Strength

230MPa

Impact

95kJ/m²

AKROLOY® PA GF 40 black (2845) is a 40% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state. The advanced version of this Product is AKROLOY® PA GF 40 black (6416) with a modern stabilization technology, featuring improved weld-line strength and an even wider process window.

AKROMID®

A3 GF 30 4 black (3571)

PA66 GF30

A3 GF 30 4 black (3571) - PA 6.6 30% glass fiber reinforced, hydrolysis and chemically stabilised, suitable for cooling systems in the automotive industry


Modulus

11.500MPa

Strength

210MPa

Impact

80kJ/m²

A3 GF 30 4 black (3571) - PA 6.6 30% glass fiber reinforced, hydrolysis and chemically stabilised, suitable for cooling systems in the automotive industry

AKROMID®

B3 1 L black (4525)

PA6+PP

AKROMID® B3 1 L schwarz (4525) - PA/PP-Blend lightweight, cost reduced


Modulus

2.300MPa

Strength

55MPa

Impact

180kJ/m²

AKROMID® B3 1 L schwarz (4525) - PA/PP-Blend lightweight, cost reduced

AKROMID®

B3 1 L natural (4685)

PA6 + PP

AKROMID® B3 1 L natural (4685)- unreinforced PA6/PP-Blend lightweight, cost reduced


Modulus

2.400MPa

Strength

55MPa

Impact

180kJ/m²

AKROMID® B3 1 L natural (4685)- unreinforced PA6/PP-Blend lightweight, cost reduced

AKROMID®

S3 8 natural (4881)

PA610

AKROMID® S3 8 natural (4881) - partly bio-based PA 6.10, low moisture absorption, increased chemical resistance, food contact


Modulus

2.300MPa

Strength

65MPa

Impact

180kJ/m²

AKROMID® S3 8 natural (4881) - partly bio-based PA 6.10, low moisture absorption, increased chemical resistance, food contact

AKROMID®

Preliminary

T9 GF 15 S1 black (7820)

PPA-I GF15

AKROMID® T9 GF 15 S1 black (7820) is a 15% glass fibre reinforced, cold impact strength polyphthalamide with medium stiffness and strength, as well as high chemical resistance. The compound is based on PA9T and has lower moisture uptake than conventional PA6T variants. This leads to a significantly higher consistency of the glass transition temperature and higher strength at elevated temperatures especially in conditioned state.


Modulus

5.000MPa

Strength

120MPa

Impact

73kJ/m²

AKROMID® T9 GF 15 S1 black (7820) is a 15% glass fibre reinforced, cold impact strength polyphthalamide with medium stiffness and strength, as well as high chemical resistance. The compound is based on PA9T and has lower moisture uptake than conventional PA6T variants. This leads to a significantly higher consistency of the glass transition temperature and higher strength at elevated temperatures especially in conditioned state.

AKROMID®

A3 1 S3 grey (2955)

PA66+PA6-I

AKROMID® A3 1 S3 grey (2955) - PA 6.6, unreinforced, impact modified, for connecting and fixing systems, automotive, E&E


Modulus

2.500MPa

Strength

68MPa

Impact

180kJ/m²

AKROMID® A3 1 S3 grey (2955) - PA 6.6, unreinforced, impact modified, for connecting and fixing systems, automotive, E&E

158596080

AKROMID®

Preliminary

A3 black (7557)PA66

AKROMID® A3 black (7557) is an unreinforced, UV stabilised polyamide 6.6.

Properties

Modulus

3.200MPa

Strength

80MPa

Impact

180kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
3200 MPa
1200 MPa

Tensile stress at yield

ISO 527-2

50 mm/min | d.a.m.
50 mm/min | conditioned
80 MPa
45 MPa

Tensile strain at break

ISO 527-2

50 mm/min | d.a.m.
50 mm/min | conditioned
> 10 %
> 25 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
30°C | conditioned
-
no break
no break
no break
no break

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
4 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
65 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
210 °C

Temperature of deflection under load HDT/C

ISO 75

8 MPa
45 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
262 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

General properties


Density

ISO 1183

23°C
1,14 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
2,9 %

Molding shrinkage

ISO 294-4

flow
transverse
1,3 - 1,5 %
1,5 - 1,7 %

Rheological Properties


Flowability

AKRO

1 mm Thickness
2 mm Thickness
310 mm
980 mm

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more