A3 1 S3 15 natural (2892)

PA66-I

AKROMID® A3 1 S3 15 natural (2892) - PA66, unreinforced, impact modified, good flowability, for connecting and fixing systems, automotive, E&E


Modulus

2.700MPa

Strength

63MPa

Impact

180kJ/m²

AKROMID® A3 1 S3 15 natural (2892) - PA66, unreinforced, impact modified, good flowability, for connecting and fixing systems, automotive, E&E

AKROLOY®

PA LGF 50 natural (5504)

PA66+PA6I/6T LGF50

AKROLOY® PA LGF 50 natural (5504) - Semi-aromatic polyamide blend, 50% long glass fiber reinforced, low shrinkage, very good fatigue performance


Modulus

19.000MPa

Strength

290MPa

Impact

100kJ/m²

AKROLOY® PA LGF 50 natural (5504) - Semi-aromatic polyamide blend, 50% long glass fiber reinforced, low shrinkage, very good fatigue performance

AKROMID®

D3 CGM 15/20 S1 black (6284)

PA612 (CF15+GF20)

AKROMID® D3 CGM 15/20 S1 black (6284) - PA 6.12, carbon fiber, glass fiber, impact modified, connector, electrical conductivity


Modulus

13.500MPa

Strength

145MPa

Impact

80kJ/m²

AKROMID® D3 CGM 15/20 S1 black (6284) - PA 6.12, carbon fiber, glass fiber, impact modified, connector, electrical conductivity

AKROMID®

UL

B3 GF 30 FR black (7459)

PA6 GF30 FR(40)

AKROMID® B3 GF 30 FR black (7459) is an at UL in all colors listed PA6 with 30% glass-fibers and flame retardant free of halogens and red phosphorus.


Modulus

10.800MPa

Strength

135MPa

Impact

65kJ/m²

AKROMID® B3 GF 30 FR black (7459) is an at UL in all colors listed PA6 with 30% glass-fibers and flame retardant free of halogens and red phosphorus.

AKROMID®

B28 GM 10/20 1 LT black (7749)

PA6 (GF10+GB20)

AKROMID® B28 GM 10/20 1 LT black (7749) is a 10% glass fibre reinforced, 20% glass bead filled, heat stabilised, lasertransparent and laser markable polyamide 6 with good surface and low warpage


Modulus

6.300MPa

Strength

110MPa

Impact

40kJ/m²

AKROMID® B28 GM 10/20 1 LT black (7749) is a 10% glass fibre reinforced, 20% glass bead filled, heat stabilised, lasertransparent and laser markable polyamide 6 with good surface and low warpage

AKROMID®

C28 M 30 6 black (7934)

PA66+PA6 MD30

AKROMID® C28 M 30 6 black (7934) is a 30% mineral filled, high heat stabilized polyamid 6.6/6 with very good surface low warpage and easy flow.


Modulus

6.000MPa

Strength

70MPa

Impact

30kJ/m²

AKROMID® C28 M 30 6 black (7934) is a 30% mineral filled, high heat stabilized polyamid 6.6/6 with very good surface low warpage and easy flow.

AKROMID®

UL

C3 1 FR natural (8050)

PA66+PA6 FR(30)

AKROMID® C3 1 FR natural (8050) - PA6/6.6 blend, unreinforced, flame retardant, UL-listed, very good flowability, public transportation, new mobility.


Modulus

3.600MPa

Strength

77MPa

Impact

100kJ/m²

AKROMID® C3 1 FR natural (8050) - PA6/6.6 blend, unreinforced, flame retardant, UL-listed, very good flowability, public transportation, new mobility.

138394080

AKROMID®

B28 GF 15 1 S3 black (7514)PA6-I GF15

Our AKROMID® B28 GF 15 1 S3 black (7514) is a 15% glass fibre reinforced, heat stabilised polyamide 6 which offers medium stiffness and strength, making it the go-to material for elevated tremperature applications, for example in industrial engineering or automotive industry. Furthermore, it is not only easy flowing, making it easy to process, but also impact modified, exceeding the impact resistance of standard PA GF 15.

Features

heat stabilised 130
impact modified
easy flow
process improved

Properties

Modulus

5.000MPa

Strength

110MPa

Impact

70kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
5000 MPa
2500 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
110 MPa
75 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
4,4 %
> 10 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
70 kJ/m²
95 kJ/m²
45 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
30°C | d.a.m.
-
7 kJ/m²
5 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
215 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
225 °C

Flammability


Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,23 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,2 - 0,4 %
0,6 - 0,8 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more