Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROMID®

B3 GK 50 natural (3690)

PA6 GB50

AKROMID® B3 GK 50 natural (3690) - PA 6, 50% glass beads reinforced, good surface, low warpage


Modulus

5.700MPa

Strength

75MPa

Impact

42kJ/m²

AKROMID® B3 GK 50 natural (3690) - PA 6, 50% glass beads reinforced, good surface, low warpage

AKROMID®

B3 GF 60 1 black (4644)

PA6 GF60

AKROMID® B3 GF 60 1 black (4644) - 60% glass fiber reinforced, PA 6, heat stabilised, easy flow


Modulus

21.000MPa

Strength

250MPa

Impact

90kJ/m²

AKROMID® B3 GF 60 1 black (4644) - 60% glass fiber reinforced, PA 6, heat stabilised, easy flow

AKROMID®

UL

C3 1 FR black (5266)

PA66+PA6 FR (30)

AKROMID® C3 1 FR black (5266) - PA6/6.6 blend, unreinforced, flame retardant, UL-listed, good flowability, public transportation, new mobility.


Modulus

3.400MPa

Strength

75MPa

Impact

100kJ/m²

AKROMID® C3 1 FR black (5266) - PA6/6.6 blend, unreinforced, flame retardant, UL-listed, good flowability, public transportation, new mobility.

AKROLOY®

Preliminary

PA GF 30 natural (6412)

PA66+PA6I/6T GF30

AKROLOY® PA GF 30 natur (6412) is a 30% glass fibre reinforced, semi-aromatic polyamide blend with high stiffness and strength, even in conditioned state.


Modulus

10.200MPa

Strength

200MPa

Impact

70kJ/m²

AKROLOY® PA GF 30 natur (6412) is a 30% glass fibre reinforced, semi-aromatic polyamide blend with high stiffness and strength, even in conditioned state.

AKROMID®

A3 GF 30 3 black (21005)

PA66 GF30

AKROMID® A3 GF 30 3 black (21005) - PA 6.6 30% glass fiber reinforced, inorganic heat stabilised, nucleated, technical parts in industrial engineering and in the automotive industry


Modulus

10.000MPa

Strength

170MPa

Impact

55kJ/m²

AKROMID® A3 GF 30 3 black (21005) - PA 6.6 30% glass fiber reinforced, inorganic heat stabilised, nucleated, technical parts in industrial engineering and in the automotive industry

AKROMID®

B3 GF 30 2 S1 grey (4289)

PA6-I GF30

AKROMID® B3 GF 30 2 S1 grey (4289) - PA 6, 30% glass fiber reinforced, impact modified and UV stabilised, for industrial applications, housings and covers, automotive


Modulus

8.500MPa

Strength

120MPa

Impact

65kJ/m²

AKROMID® B3 GF 30 2 S1 grey (4289) - PA 6, 30% glass fiber reinforced, impact modified and UV stabilised, for industrial applications, housings and covers, automotive

AKROMID®

B3 GF 15 1 black (2482)

PA6 GF15

AKROMID® B3 GF 15 1 black (2482) is a 15% glass fibre reinforced, heat stabilised polyamide 6 with medium stiffness and strength.


Modulus

6.100MPa

Strength

120MPa

Impact

52kJ/m²

AKROMID® B3 GF 15 1 black (2482) is a 15% glass fibre reinforced, heat stabilised polyamide 6 with medium stiffness and strength.

132333480

AKROTEK®

Preliminary

PK-VM GF 50 8 natural (6989)PK GF50

AKROTEK® PK-VM GF 50 8 natural (6989) is a 15% glass fibre reinforced polyketone with very high stiffness and strength. PK is characterized by its outstanding media resistance, which qualifies it to be used for components that are in contact with chemicals. The material corresponds to the European food guideline EU 10/2011 and to the American FDA 21 CFR. This grade is suitable for parts of kitchen and household appliances. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61.

Features

hydrolysis / chemically stabilised

Regulatory

eu102011fda

Properties

Modulus

14.000MPa

Strength

160MPa

Impact

60kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
14000 MPa
13500 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
160 MPa
150 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
1,7 %
1,7 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
60 kJ/m²
55 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
15 kJ/m²
15 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
220 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,65 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
0,4 - 0,5 %

Molding shrinkage

ISO 294-4

flow
transverse
0,1 - 0,3 %
0,4 - 0,6 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more