HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROTEK®

Preliminary

PK-VM GF 10 natural (8679)

PK GF10

AKROTEK® PK-VM GF 10 natural (8679) - Polyketon, 10% glass fibre reinforced, chemical and hydrolysis resistance


Modulus

3.600MPa

Strength

75MPa

Impact

61kJ/m²

AKROTEK® PK-VM GF 10 natural (8679) - Polyketon, 10% glass fibre reinforced, chemical and hydrolysis resistance

AKROTEK®

Preliminary

PPS CF 30 black (8612)

PPS CF30

AKROTEK® PPS CF 30 black (8612) is a 30% carbon fibre reinforced, Polyphenylene sulfide with high rigidity and strength, as well as high temperature and chemical resistance.


Modulus

28.000MPa

Strength

230MPa

Impact

35kJ/m²

AKROTEK® PPS CF 30 black (8612) is a 30% carbon fibre reinforced, Polyphenylene sulfide with high rigidity and strength, as well as high temperature and chemical resistance.

AKROTEK®

Preliminary

PK-VM GF 15 natural (8680)

PK GF15

AKROTEK® PK-VM GF 15 natural (8680) - Polyketon, 15% glass fiber reinforced, chemical and hydrolysis resistance


Modulus

4.600MPa

Strength

100MPa

Impact

65kJ/m²

AKROTEK® PK-VM GF 15 natural (8680) - Polyketon, 15% glass fiber reinforced, chemical and hydrolysis resistance

AKROMID®

B3 GF 30 1 grey (7574)

PA6 GF30

AKROMID® B3 GF 30 1 grey (7574) is a 30% glass fibre reinforced, heat stabilised polyamide 6 with high rigidity and strength


Modulus

9.900MPa

Strength

168MPa

Impact

NA

AKROMID® B3 GF 30 1 grey (7574) is a 30% glass fibre reinforced, heat stabilised polyamide 6 with high rigidity and strength

AKROTEK®

Preliminary

PK-VM GF 20 natural (8681)

PK GF20

AKROTEK® PK-VM GF 20 natural (8681) - Polyketon, 20% glass fibre reinforced, chemical and hydrolysis resistance


Modulus

5.700MPa

Strength

117MPa

Impact

65kJ/m²

AKROTEK® PK-VM GF 20 natural (8681) - Polyketon, 20% glass fibre reinforced, chemical and hydrolysis resistance

AKROTEK®

Preliminary

AM ICF 20 black (8723)

ASACF20

AKROTEK® AM ICF 20 black (8723) - recycled carbon fibre reinforced for additive manufacturing (3D-printing)


Modulus

13.400MPa

Strength

105MPa

Impact

25kJ/m²

AKROTEK® AM ICF 20 black (8723) - recycled carbon fibre reinforced for additive manufacturing (3D-printing)

AKROMID®

A3 S3 natural (1176)

PA66-I

AKROMID® A3 S3 natural (1176) - PA 6.6, unreinforced, dry impact modified, for connecting and fixing systems, automotive, E&E


Modulus

2.800MPa

Strength

67MPa

Impact

180kJ/m²

AKROMID® A3 S3 natural (1176) - PA 6.6, unreinforced, dry impact modified, for connecting and fixing systems, automotive, E&E

176777880

AKROMID®

UL
Preliminary

NEXT S3 GF 15 1 HU natural (8822)PA6.10 GF15

AKROMID® NEXT S3 GF 15 1 HU natural (8822) is a partially biobased and heat-stabilised PA6.10. With 15% glass fibre reinforcement, the material is suitable for household and industrial applications with medium demands on strength and stiffness. This sustainable and UL listed grade is characterised by its low moisture absorption and high chemical resistance compared to classic PA6 and PA 6.

Features

Bio-based
heat stabilised 130
reduced moisture

Regulatory

ul

Properties

Modulus

5.000MPa

Strength

110MPa

Impact

75kJ/m²

Sustainability


Biobased carbon content

61 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
5000 MPa
3500 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
110 MPa
75 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
5,5 %
15 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
75 kJ/m²
80 kJ/m²
60 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
30°C | d.a.m.
-
5 kJ/m²
5 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
190 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
220 °C

Temperature of deflection under load HDT/C

ISO 75

8 MPa
75 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

UL
0,8 mm Wall thickness
UL
3,2 mm Wall thickness
HB Class
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,18 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
1,4 - 1,6 %

Molding shrinkage

ISO 294-4

flow
transverse
0,5 - 0,7 %
1,0 - 1,2 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.