Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROLEN®

Preliminary

PP ICF 30 AM black (8344)

PP CF30

AKROLEN® PP ICF 30 AM black (8344) - recycled carbon fibre reinforced polypropylene for additive manufacturing (3D-printing)


Modulus

12.500MPa

Strength

85MPa

Impact

50kJ/m²

AKROLEN® PP ICF 30 AM black (8344) - recycled carbon fibre reinforced polypropylene for additive manufacturing (3D-printing)

AKROMID®

S3 1 black (3317)

PA610

AKROMID® S3 1 black (3317) is a nonreinforced and heat stabilised polyamide 6.10 with lower moisture absorption and high chemical resistance.


Modulus

2.400MPa

Strength

70MPa

Impact

180kJ/m²

AKROMID® S3 1 black (3317) is a nonreinforced and heat stabilised polyamide 6.10 with lower moisture absorption and high chemical resistance.

AKROTEK®

PK-HM 8 natural (6145)

PK

AKROTEK® PK-HM 8 natural (6145) - Polyketon, unreinforced, Tribology, friction and wear, chemical resistance, EU 10/2011, FDA 21 CFR


Modulus

1.400MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-HM 8 natural (6145) - Polyketon, unreinforced, Tribology, friction and wear, chemical resistance, EU 10/2011, FDA 21 CFR

AKROMID®

Preliminary

T5 8 black (6454)

PPA

AKROMID® T5 8 black (6454) - PPA, unreinforced, food contact, kitchen and household appliances, fitting, ACS, WRAS, NSF 61, EU 10/2011, FDA


Modulus

3.800MPa

Strength

75MPa

Impact

40kJ/m²

AKROMID® T5 8 black (6454) - PPA, unreinforced, food contact, kitchen and household appliances, fitting, ACS, WRAS, NSF 61, EU 10/2011, FDA

AKROTEK®

Preliminary

PK-VM GF 15 8 black (6991)

PK GF15

AKROTEK® PK-VM GF 15 8 black (6991) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

4.500MPa

Strength

95MPa

Impact

55kJ/m²

AKROTEK® PK-VM GF 15 8 black (6991) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROMID®

B3 GF 35 S1 natural (920)

PA6-I GF35

AKROMID® B3 GF 35 S1 natural (920) is a 35% glass fibre reinforced, cold impact strength polyamide 6 with high stiffness and strength and light inherent color


Modulus

11.000MPa

Strength

190MPa

Impact

80kJ/m²

AKROMID® B3 GF 35 S1 natural (920) is a 35% glass fibre reinforced, cold impact strength polyamide 6 with high stiffness and strength and light inherent color

AKROTEK®

PK-VM GF 10 grey (7344)

PK GF10

AKROTEK® PK-VM GF 10 grey (7344) - Polyketon, 10% glass fiber reinforced, chemical resistance, RAL 7044


Modulus

3.600MPa

Strength

65MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 10 grey (7344) - Polyketon, 10% glass fiber reinforced, chemical resistance, RAL 7044

173747580

AKROMID®

A3 1 S3 natural (2847)PA66-I

AKROMID® A3 1 S3 natural (2847) is an unreinforced, impact modified Polyamide 6.6. It is characterised by a medium dry impact strength. Furthermore, the material is heat stabilised and therefore perfectly suitable for connecting and fixing systems which are used at elevated temperatures in the automotive and electro industry.

Features

heat stabilised 130
impact modified

Properties

Modulus

2.500MPa

Strength

65MPa

Impact

180kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
2500 MPa
1000 MPa

Tensile stress at yield

ISO 527-2

50 mm/min | d.a.m.
50 mm/min | conditioned
65 MPa
40 MPa

Tensile strain at yield

ISO 527-2

50 mm/min | d.a.m.
4,6 %

Tensile strain at break

ISO 527-2

50 mm/min | d.a.m.
50 mm/min | conditioned
≥ 25 %
> 100 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
no break

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
40°C | d.a.m.
-
12 kJ/m²
95 kJ/m²
8 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
60 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
194 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
260 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,11 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
2,5 %

Molding shrinkage

ISO 294-4

flow
transverse
1,3 - 1,5 %
1,5 - 1,7 %

Rheological Properties


MVR

ISO 1133

275°C/5kg
55 cm³/10 min

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more