Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROLOY®

Preliminary

PA GF 60 LA black (8168)

PA66 + PA6I/6T GF60

AKROLOY® PA GF 60 LA black (8168) is a 60% glass fibre reinforced, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.


Modulus

21.400MPa

Strength

275MPa

Impact

95kJ/m²

AKROLOY® PA GF 60 LA black (8168) is a 60% glass fibre reinforced, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.

AKROMID®

B28 GF 30 S3 black (8438)

PA6-I GF30

AKROMID® B28 GF 30 S3 black (8438) - PA 6, 30% glass fiber reinforced, impact modified, industrial applications, housings and covers, automotive


Modulus

9.000MPa

Strength

155MPa

Impact

100kJ/m²

AKROMID® B28 GF 30 S3 black (8438) - PA 6, 30% glass fiber reinforced, impact modified, industrial applications, housings and covers, automotive

AKROMID®

A3 1 L natural (4800)

PA66 + PP

AKROMID® A3 1 L natural (4800) - unreinforced PA6.6/PP-Blend lightweight, cost reduced


Modulus

2.300MPa

Strength

55MPa

Impact

180kJ/m²

AKROMID® A3 1 L natural (4800) - unreinforced PA6.6/PP-Blend lightweight, cost reduced

AKROTEK®

PK-HM 8 natural (6145)

PK

AKROTEK® PK-HM 8 natural (6145) - Polyketon, unreinforced, Tribology, friction and wear, chemical resistance, EU 10/2011, FDA 21 CFR


Modulus

1.400MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-HM 8 natural (6145) - Polyketon, unreinforced, Tribology, friction and wear, chemical resistance, EU 10/2011, FDA 21 CFR

AKROTEK®

PK-VM GF 50 8 black (6936)

PK GF50

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

14.000MPa

Strength

170MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROMID®

Preliminary

NEXT 5.6 3 GF 30 S3 black (8444)

PA56 GF30

AKROMID® NEXT 5.6 3 GF 30 S3 black (8444) - partly bio-based and HMD-free PA 5.6, 30 % GF, impact modified, high strength and stiffness.


Modulus

8.600MPa

Strength

180MPa

Impact

96kJ/m²

AKROMID® NEXT 5.6 3 GF 30 S3 black (8444) - partly bio-based and HMD-free PA 5.6, 30 % GF, impact modified, high strength and stiffness.

AKROMID®

B3 GF 20 black (2491)

PA6 GF20

AKROMID® B3 GF 20 black (2491) is a 20% glass fibre reinforced polyamide 6 with medium stiffness and strength


Modulus

6.800MPa

Strength

150MPa

Impact

73kJ/m²

AKROMID® B3 GF 20 black (2491) is a 20% glass fibre reinforced polyamide 6 with medium stiffness and strength

172737480

AKROMID®

Preliminary

T9 ICF 20 6 black (7907)PPA CF 20

AKROMID® T9 ICF 20 6 black (7907) is a with 20% recycled carbon fibre reinforced polyphthalamide with high stiffness and strength, as well as high chemical resistance. The compound is based on PA9T and has lower moisture uptake than conventional PA6T variants. This leads to a significantly higher consistency of the glass transition temperature and higher strength at elevated temperatures especially in conditioned state.

Features

reduced moisture
E&E
metal substitution
Sports & leisure

Properties

Modulus

14.000MPa

Strength

190MPa

Impact

35kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
14000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
190 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
1,8 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
35 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
5 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
270 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
300 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

General properties


Density

ISO 1183

23°C
1,22 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,1 - 0,3 %
0,5 - 0,7 %

Electrical Properties


Surface resistivity

DIN EN 62631-3-2

d.a.m.
102

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more