HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROLOY®

PA GF 60 black (7789)

PA66+PA6I/6T GF60

AKROLOY® PA GF 60 black (7789) is a 60% glass fibre reinforced, easyflow, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.


Modulus

21.400MPa

Strength

290MPa

Impact

100kJ/m²

AKROLOY® PA GF 60 black (7789) is a 60% glass fibre reinforced, easyflow, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.

AKROTEK®

PK-VM GF 10 grey (7344)

PK GF10

AKROTEK® PK-VM GF 10 grey (7344) - Polyketon, 10% glass fiber reinforced, chemical resistance, RAL 7044


Modulus

3.600MPa

Strength

65MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 10 grey (7344) - Polyketon, 10% glass fiber reinforced, chemical resistance, RAL 7044

AKROMID®

Preliminary

NEXT G3 GF 30 1 L CI natural (8377)

PA6.9 + PP GF30

AKROMID® NEXT G3 GF 30 1 L CI natural (8377) - PA 6.9/PP blend, bio-based, certified, low moisture absorption, weight reduction.


Modulus

8.000MPa

Strength

125MPa

Impact

65kJ/m²

AKROMID® NEXT G3 GF 30 1 L CI natural (8377) - PA 6.9/PP blend, bio-based, certified, low moisture absorption, weight reduction.

AKROMID®

Preliminary

C3 GF 30 8 black (5657)

PA66 + PA6 GF30

AKROMID® C3 GF 30 8 black (5657) - PA6.6/6 Blend, GF 30, FDA, EU 10/2010, food contact, kitchen and household appliances


Modulus

9.400MPa

Strength

190MPa

Impact

82kJ/m²

AKROMID® C3 GF 30 8 black (5657) - PA6.6/6 Blend, GF 30, FDA, EU 10/2010, food contact, kitchen and household appliances

AKROTEK®

Preliminary

PK-VM GF 20 natural (8681)

PK GF20

AKROTEK® PK-VM GF 20 natural (8681) - Polyketon, 20% glass fibre reinforced, chemical and hydrolysis resistance


Modulus

5.700MPa

Strength

117MPa

Impact

65kJ/m²

AKROTEK® PK-VM GF 20 natural (8681) - Polyketon, 20% glass fibre reinforced, chemical and hydrolysis resistance

AKROMID®

B3 GF 35 S1 natural (920)

PA6-I GF35

AKROMID® B3 GF 35 S1 natural (920) is a 35% glass fibre reinforced, cold impact strength polyamide 6 with high stiffness and strength and light inherent color


Modulus

11.000MPa

Strength

190MPa

Impact

80kJ/m²

AKROMID® B3 GF 35 S1 natural (920) is a 35% glass fibre reinforced, cold impact strength polyamide 6 with high stiffness and strength and light inherent color

AKROMID®

Preliminary

NEXT U3 ICF 20 1 black (8232)

PA11 CF20

AKROMID® NEXT U3 ICF 20 1 black (8232) - PA11 made of renewable raw materials, recycled carbon fibre, low density, Fused Filament Fabrication


Modulus

9.300MPa

Strength

110MPa

Impact

60kJ/m²

AKROMID® NEXT U3 ICF 20 1 black (8232) - PA11 made of renewable raw materials, recycled carbon fibre, low density, Fused Filament Fabrication

172737480

AKROMID®

Preliminary

B28 GF 30 natural (6941)PA 6 GF 30

AKROMID B28 GF 30 natural (6941) is a 30% glass fibre reinforced, easy flowing PA6. Due to its very good flowability, this grade has a good surface. It complies with the bus fire standard ECE R 118.03 annex 6 and 8 and is suitable for panels, seat shells, armrests and footrests where high stiffness and strength is required. The material is easy to colour.

Features

easy flow

Regulatory

ece11803

Properties

Modulus

10.200MPa

Strength

180MPa

Impact

80kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
10200 MPa
6200 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
180 MPa
102 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
3 %
5,5 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
8400 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
230 MPa

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
80 kJ/m²
87 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
210 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
220 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

0,4 mm Wall thickness
0,8 mm Wall thickness
1,6 mm Wall thickness
3,2 mm Wall thickness
HB Class
HB Class
HB Class
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

Protection Bus

ECE 118

Appendix 6, 8

General properties


Density

ISO 1183

23°C
1,35 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,1 - 0,3 %
0,5 - 0,7 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more