HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/mĀ²
558 Compounds found
Recommended Ā 
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

PRECITEĀ®

Preliminary

P3 GF 25 9 FR natural (8212)

PBT GF25 FR(40)

PRECITEĀ® P3 GF 25 9 FR natural (8212) - PBT, 25% glass fiber, flame retardant, high stiffness and strength, good long-term heat-aging, E-Mobility, E&E industry.


Modulus

8.500MPa

Strength

123MPa

Impact

53kJ/mĀ²

PRECITEĀ® P3 GF 25 9 FR natural (8212) - PBT, 25% glass fiber, flame retardant, high stiffness and strength, good long-term heat-aging, E-Mobility, E&E industry.

AKROMIDĀ®

A3 CF 20 black (3132)

PA66 CF20

AKROMIDĀ® A3 CF 20 black (3132) is a 20% carbon fibre reinforced polyamide 6.6 with high flexural strength and good sliding properties


Modulus

15.000MPa

Strength

200MPa

Impact

40kJ/mĀ²

AKROMIDĀ® A3 CF 20 black (3132) is a 20% carbon fibre reinforced polyamide 6.6 with high flexural strength and good sliding properties

AKROMIDĀ®

A3 1 L natural (4800)

PA66 + PP

AKROMIDĀ® A3 1 L natural (4800) - unreinforced PA6.6/PP-Blend lightweight, cost reduced


Modulus

2.300MPa

Strength

55MPa

Impact

180kJ/mĀ²

AKROMIDĀ® A3 1 L natural (4800) - unreinforced PA6.6/PP-Blend lightweight, cost reduced

AKROLOYĀ®

Preliminary

PA GF 30 black (6415)

PA66+PA6I/6T GF30

AKROLOYĀ® PA GF 30 black (6415) is a 30% glass fibre reinforced, semi-aromatic polyamide blend with high stiffness and strength, even in conditioned state.


Modulus

9.800MPa

Strength

200MPa

Impact

65kJ/mĀ²

AKROLOYĀ® PA GF 30 black (6415) is a 30% glass fibre reinforced, semi-aromatic polyamide blend with high stiffness and strength, even in conditioned state.

AKROMIDĀ®

UL

B3 1 black (6528)

PA6

AKROMIDĀ® B3 1 black (6528) is an unreinforced, heat stabilised polyamide 6


Modulus

3.600MPa

Strength

85MPa

Impact

180kJ/mĀ²

AKROMIDĀ® B3 1 black (6528) is an unreinforced, heat stabilised polyamide 6

PRECITEĀ®

Preliminary

P3 GF 40 natural (6943)

PBT GF 40

PRECITEĀ® P3 GF 40 natural (6943) is a 40% glass fibre reinforced, medium viscous poly(butylene terephthalate) (PBT) with very high stiffness and toughness as well as high dimensional and chemical resistance.


Modulus

13.500MPa

Strength

175MPa

Impact

70kJ/mĀ²

PRECITEĀ® P3 GF 40 natural (6943) is a 40% glass fibre reinforced, medium viscous poly(butylene terephthalate) (PBT) with very high stiffness and toughness as well as high dimensional and chemical resistance.

AKROLOYĀ®

PA GF 50 white (5137)

PA66+PA6I/6T GF50

AKROLOYĀ® PA GF 50 white (5137) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.


Modulus

20.000MPa

Strength

250MPa

Impact

105kJ/mĀ²

AKROLOYĀ® PA GF 50 white (5137) is a 50% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.

172737480

AKROTEKĀ®

PK-VM ICF 15 black (6074)PK CF15

AKROTEKĀ® PK-VM ICF 15 black (6074) is a 15% carbon fibre reinforced polyketon with good sliding properties.

Features

hydrolysis / chemically stabilised

Properties

Modulus

9.000MPa

Strength

90MPa

Impact

30kJ/mĀ²

Sustainability


Recycled content

15 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
9000 MPa
8800 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
90 MPa
90 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
1,5 %
1,5 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
8600 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
120 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
2 %

Charpy impact strength

ISO 179-1/1eU

23Ā°C | d.a.m.
23Ā°C | conditioned
30 kJ/mĀ²
30 kJ/mĀ²

Thermal Properties


Melting temperature

ISO 11357-3

DSC, 10K/min
220 Ā°C

General properties


Density

ISO 1183

23Ā°C
1,26 g/cmĀ³

Humidity absorption

ISO 1110

70Ā°C, 62% r.H.
0,7 - 0,8 %

Molding shrinkage

ISO 294-4

flow
transverse
0,4 - 0,6 %
1,0 - 1,2 %

Electrical Properties


Surface resistivity

DIN EN 62631-3-2

d.a.m.
104 ā„¦

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKROĀ®, AKROMIDĀ®, AKROLENĀ®, AKROLOYĀ®, AKROTEKĀ®, ICXĀ® and PRECITEĀ® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more