HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROMID®

A3 GF 50 4 black (7282)

PA66 GF50

AKROMID® A3 GF 50 4 black (7282) is a 50% glass fibre reinforced, hydrolysis/chemical stabilised polyamide 6.6 with very high rigidity and strength


Modulus

17.000MPa

Strength

250MPa

Impact

110kJ/m²

AKROMID® A3 GF 50 4 black (7282) is a 50% glass fibre reinforced, hydrolysis/chemical stabilised polyamide 6.6 with very high rigidity and strength

AKROLEN®

Preliminary

PP ICF 30 AM black (8344)

PP CF30

AKROLEN® PP ICF 30 AM black (8344) - recycled carbon fibre reinforced polypropylene for additive manufacturing (3D-printing)


Modulus

12.500MPa

Strength

85MPa

Impact

50kJ/m²

AKROLEN® PP ICF 30 AM black (8344) - recycled carbon fibre reinforced polypropylene for additive manufacturing (3D-printing)

AKROMID®

UL

B3 GF 35 1 HU red (8416)

PA6 GF35

AKROMID® B3 GF 35 1 HU red (8416) - PA 6, 35% glass fibre, heat ageing resistant, high rigidity and strength, UL listed HB.


Modulus

12.000MPa

Strength

190MPa

Impact

NA

AKROMID® B3 GF 35 1 HU red (8416) - PA 6, 35% glass fibre, heat ageing resistant, high rigidity and strength, UL listed HB.

AKROMID®

B3 GF 30 1 grey (7574)

PA6 GF30

AKROMID® B3 GF 30 1 grey (7574) is a 30% glass fibre reinforced, heat stabilised polyamide 6 with high rigidity and strength


Modulus

9.900MPa

Strength

168MPa

Impact

NA

AKROMID® B3 GF 30 1 grey (7574) is a 30% glass fibre reinforced, heat stabilised polyamide 6 with high rigidity and strength

AKROMID®

A3 GF 40 1 L black (4671)

PA66+PP GF40

AKROMID® A3 GF 40 1 L black (4671) - PA6.6/PP-Blend, 40% glass fibre reinforced, lower density, cost reduced, zinc chloride


Modulus

11.800MPa

Strength

170MPa

Impact

80kJ/m²

AKROMID® A3 GF 40 1 L black (4671) - PA6.6/PP-Blend, 40% glass fibre reinforced, lower density, cost reduced, zinc chloride

AKROMID®

B3 GF 30 8 natural (5663)

PA6 GF30

AKROMID® B3 GF 30 8 natural (5663) - PA6, 30% glass fiber, food contact, kitchen and household appliances


Modulus

10.000MPa

Strength

185MPa

Impact

95kJ/m²

AKROMID® B3 GF 30 8 natural (5663) - PA6, 30% glass fiber, food contact, kitchen and household appliances

AKROTEK®

PK-VM 8 black (6466)

PK

AKROTEK® PK-VM 8 black (6466) - Polyketon, Tribology, friction and wear, chemical resistance, food, drinking water, EU 10/2011


Modulus

1.600MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-VM 8 black (6466) - Polyketon, Tribology, friction and wear, chemical resistance, food, drinking water, EU 10/2011

171727380

AKROMID®

Internal

S3 GF 50 1 natural (3533)PA610 GF50

AKROMID® S3 GF 50 1 natural (3533) is a 50% glass fibre reinforced, heat stabilised polyamide 6.10 with very high stiffness and strength as well as lower moisture absorption, high chemical resistance and light inherent color.

Features

heat stabilised 130
reduced moisture

Properties

Modulus

14.500MPa

Strength

200MPa

Impact

100kJ/m²

Sustainability


Biobased carbon content

61 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
14500 MPa
11000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
200 MPa
150 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
3,5 %
4,5 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
13800 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
310 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
3,6 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
30°C | d.a.m.
-
100 kJ/m²
100 kJ/m²
105 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
30°C | d.a.m.
-
20 kJ/m²
16 kJ/m²

Ball indentation hardness

ISO 2039-1

961N/30s | d.a.m.
230 MPa

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
205 °C

Temperature of deflection under load HDT/C

ISO 75

8 MPa
170 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

UL
0,8 mm Wall thickness
UL
3,2 mm Wall thickness
HB Class
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,51 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
0,9 %

Molding shrinkage

ISO 294-4

flow
transverse
0,3 %
1,0 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.