AKROMID®

UL
Preliminary

B3 GF 30 1 HU LA black (2862)

PA6 GF30

AKROMID® B3 GF 30 1 HU LA black (2862) - PA 6, 30% glass fibre, heat ageing resistant, high rigidity and strength, UL listed HB, laser markable, automotive, E&E, industry.


Modulus

10.300MPa

Strength

185MPa

Impact

95kJ/m²

AKROMID® B3 GF 30 1 HU LA black (2862) - PA 6, 30% glass fibre, heat ageing resistant, high rigidity and strength, UL listed HB, laser markable, automotive, E&E, industry.

AKROMID®

B28 GF 30 S3 black (8438)

PA6-I GF30

AKROMID® B28 GF 30 S3 black (8438) - PA 6, 30% glass fiber reinforced, impact modified, industrial applications, housings and covers, automotive


Modulus

9.000MPa

Strength

155MPa

Impact

100kJ/m²

AKROMID® B28 GF 30 S3 black (8438) - PA 6, 30% glass fiber reinforced, impact modified, industrial applications, housings and covers, automotive

AKROMID®

B3 GF 60 1 natural (2468)

PA6 GF60

AKROMID® B3 GF 60 1 natural (2468) is a 60% glass fibre reinforced heat stabilised polyamide 6 with very high rigidity and strength and light inherent color.


Modulus

21.000MPa

Strength

240MPa

Impact

90kJ/m²

AKROMID® B3 GF 60 1 natural (2468) is a 60% glass fibre reinforced heat stabilised polyamide 6 with very high rigidity and strength and light inherent color.

AKROMID®

B3 GF 60 black (2497)

PA6 GF60

AKROMID® B3 GF 60 black (2497) is a 60% glass fibre reinforced polyamide 6 with very high rigidity and strength


Modulus

21.000MPa

Strength

240MPa

Impact

90kJ/m²

AKROMID® B3 GF 60 black (2497) is a 60% glass fibre reinforced polyamide 6 with very high rigidity and strength

AKROMID®

A3 GFM 25/15 1 black (3335)

PA66 (GF25+MD15)

AKROMID® A3 GFM 25/15 1 black (3335) is a 25% glass fibre reinforced, 15% mineral filled, heat stabilised polyamide 6.6 with good surface and dimensional stability


Modulus

10.000MPa

Strength

150MPa

Impact

50kJ/m²

AKROMID® A3 GFM 25/15 1 black (3335) is a 25% glass fibre reinforced, 15% mineral filled, heat stabilised polyamide 6.6 with good surface and dimensional stability

AKROMID®

S3 GF 30 4 natural (3552)

PA6.10

AKROMID® S3 GF 30 4 natural (3552) is a 30% glass fibre reinforced and hydrolysis stabilised polyamide 6.10 with high stiffness and strength as well as lower moisture absorption and very high chemical resistance


Modulus

8.600MPa

Strength

160MPa

Impact

110kJ/m²

AKROMID® S3 GF 30 4 natural (3552) is a 30% glass fibre reinforced and hydrolysis stabilised polyamide 6.10 with high stiffness and strength as well as lower moisture absorption and very high chemical resistance

AKROMID®

B3 GF 50 9 RM-M natural (3698)

PA6 + X GF50

AKROMID® B3 GF 50 9 RM-M natural (3698) is a 50% glass fibre reinforced, process improved polyamide 6 with very high stiffness and strength, limited moisture absorption and light inherent color.


Modulus

16.000MPa

Strength

210MPa

Impact

70kJ/m²

AKROMID® B3 GF 50 9 RM-M natural (3698) is a 50% glass fibre reinforced, process improved polyamide 6 with very high stiffness and strength, limited moisture absorption and light inherent color.

170717280

AKROMID®

A3 GK 30 6 natural (6774)PA66 GB30

AKROMID® A3 GK 30 6 natural (6774) is a 30% glass beads filled and inorganic high temperature stabilised PA6.6. It is characterized by a high surface quality and low tendency to warp, which makes it suitable for use in technically demanding components in mechanical engineering and in the automotive industry.

Features

heat stabilised 160
recycled content
low warpage

Properties

Modulus

4.600MPa

Strength

90MPa

Impact

25kJ/m²

Sustainability


Recycled content

30 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
4600 MPa
2000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
90 MPa
52 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
≥ 4 %
25 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
4400 MPa
2000 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
135 MPa
70 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
2 mm/min | conditioned
8 %
14 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
25 kJ/m²
170 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
4,5 kJ/m²
5 kJ/m²

Thermal Properties


Melting temperature

ISO 11357-3

DSC, 10K/min
262 °C

General properties


Density

ISO 1183

23°C
1,36 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
1,9 - 2,1 %

Molding shrinkage

ISO 294-4

flow
transverse
1,1 %
1,3 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more