HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROMID®

Preliminary

S3 GF 30 4 black (3429)

PA610 GF30

AKROMID® S3 GF 30 4 black (3429) is a 30% glass fibre reinforced and hydrolysis stabilised polyamide 6.10 with high stiffness and strength as well as lower moisture absorption and very high chemical resistance.


Modulus

8.600MPa

Strength

160MPa

Impact

110kJ/m²

AKROMID® S3 GF 30 4 black (3429) is a 30% glass fibre reinforced and hydrolysis stabilised polyamide 6.10 with high stiffness and strength as well as lower moisture absorption and very high chemical resistance.

AKROMID®

C3 GF 60 1 black (4659)

PA66 + PA6 GF60

AKROMID® C3 GF 60 1 black (4659) is a 60% glass fibre reinforced, heat stabilised polyamide 6.6/6 - Blend.


Modulus

21.300MPa

Strength

270MPa

Impact

96kJ/m²

AKROMID® C3 GF 60 1 black (4659) is a 60% glass fibre reinforced, heat stabilised polyamide 6.6/6 - Blend.

AKROTEK®

Preliminary

PK-VM GF 15 8 black (6991)

PK GF15

AKROTEK® PK-VM GF 15 8 black (6991) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

4.500MPa

Strength

95MPa

Impact

55kJ/m²

AKROTEK® PK-VM GF 15 8 black (6991) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROMID®

S3 1 black (3317)

PA610

AKROMID® S3 1 black (3317) is a nonreinforced and heat stabilised polyamide 6.10 with lower moisture absorption and high chemical resistance.


Modulus

2.400MPa

Strength

70MPa

Impact

180kJ/m²

AKROMID® S3 1 black (3317) is a nonreinforced and heat stabilised polyamide 6.10 with lower moisture absorption and high chemical resistance.

AKROMID®

A3 GF 25 3 black (3094)

PA66 GF25

AKROMID® A3 GF 25 3 black (3094) is a 25% glass fibre reinforced, nucleated polyamide 6.6 with high stiffness and strength


Modulus

8.500MPa

Strength

160MPa

Impact

50kJ/m²

AKROMID® A3 GF 25 3 black (3094) is a 25% glass fibre reinforced, nucleated polyamide 6.6 with high stiffness and strength

AKROTEK®

PK-HM 8 black (6246)

PK

AKROTEK® PK-HM 8 black (6246) is an unreinforced, high viscosity polyketone. The material is suitable for drinking water contact and meets the requirements according to ACS and WRAS. Moreover the material corresponds to the European food guideline EU 10/2011, but not to the American FDA 21 CFR.


Modulus

1.600MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-HM 8 black (6246) is an unreinforced, high viscosity polyketone. The material is suitable for drinking water contact and meets the requirements according to ACS and WRAS. Moreover the material corresponds to the European food guideline EU 10/2011, but not to the American FDA 21 CFR.

AKROTEK®

Preliminary

PK-VM GF 15 8 natural (6324)

PK GF15

AKROTEK® PK-VM GF 15 8 natural (6324) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

4.500MPa

Strength

95MPa

Impact

55kJ/m²

AKROTEK® PK-VM GF 15 8 natural (6324) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

170717280

AKROLEN®

PP GFM 25/15 LA black (3143)PP (GF25+MD15)

AKROLEN® PP GFM 25/15 LA black (3143) is a 25% glass fibre reinforced, 15% mineralfilled, laser markable polypropylene with good surface and dimensional stability. This material is mainly used for thin wall housings for electronic parts in the automotive industry.

Features

laser markable
surface modified
low warpage

Properties

Modulus

6.500MPa

Strength

Na

Impact

45kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
6500 MPa

Tensile stress at break

ISO 527-2

50 mm/min | d.a.m.
75 MPa

Tensile strain at break

ISO 527-2

50 mm/min | d.a.m.
3,5 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
6600 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
105 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
3,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
30°C | d.a.m.
-
45 kJ/m²
45 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
10 kJ/m²

Izod impact strength

ISO 180/1A

23°C | d.a.m.
10 kJ/m²

Ball indentation hardness

ISO 2039-1

358N/30s | d.a.m.
100 MPa

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
150 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
163 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
167 °C

Coefficient of linear thermal expansion

ISO 11359-1/2

23°C to 80°C | parallel
23°C to 80°C | transverse
0,2 10⁻⁴/K
1,25 10⁻⁴/K

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,21 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,1 - 0,3 %
0,4 - 0,6 %

Electrical Properties


Comparative tracking index

IEC 60112

Test liquid A
600 V

Dielectric strength

IEC 60243

3 mm
18 kV/mm

Rheological Properties


MVR

ISO 1133

230°C/2,16kg
13,5 cm³/10 min

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more