AKROMID®

B3 1 natural (2499)

PA6

AKROMID® B3 1 natural (2499) is an unreinforced, heat stabilised polyamide 6 with light inherent color


Modulus

3.600MPa

Strength

85MPa

Impact

180kJ/m²

AKROMID® B3 1 natural (2499) is an unreinforced, heat stabilised polyamide 6 with light inherent color

AKROMID®

B3 GF 30 8 natural (5663)

PA6 GF30

AKROMID® B3 GF 30 8 natural (5663) - PA6, 30% glass fiber, food contact, kitchen and household appliances


Modulus

10.000MPa

Strength

185MPa

Impact

95kJ/m²

AKROMID® B3 GF 30 8 natural (5663) - PA6, 30% glass fiber, food contact, kitchen and household appliances

AKROLOY®

Preliminary

PA GF 40 natural (6413)

PA66+PA6I/6T GF40

AKROLOY® PA GF 40 natural (6413) is a 40% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.


Modulus

13.000MPa

Strength

235MPa

Impact

95kJ/m²

AKROLOY® PA GF 40 natural (6413) is a 40% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.

AKROTEK®

Preliminary

PK-VM GF 50 8 natural (6989)

PK GF50

AKROTEK® PK-VM GF 50 8 natural (6989) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

14.000MPa

Strength

160MPa

Impact

60kJ/m²

AKROTEK® PK-VM GF 50 8 natural (6989) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)

PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.


Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

AKROMID®

Preliminary

NEXT G3 GF 30 1 L CR black (8314)

PA6.9 + PP GF30

AKROMID® NEXT G3 GF 30 1 L CI black (8314) - PA 6.9/PP blend, bio-based, certified, low moisture absorption, weight reduction.


Modulus

8.000MPa

Strength

125MPa

Impact

65kJ/m²

AKROMID® NEXT G3 GF 30 1 L CI black (8314) - PA 6.9/PP blend, bio-based, certified, low moisture absorption, weight reduction.

AKROMID®

B3 GF 60 1 natural (2468)

PA6 GF60

AKROMID® B3 GF 60 1 natural (2468) is a 60% glass fibre reinforced heat stabilised polyamide 6 with very high rigidity and strength and light inherent color.


Modulus

21.000MPa

Strength

240MPa

Impact

90kJ/m²

AKROMID® B3 GF 60 1 natural (2468) is a 60% glass fibre reinforced heat stabilised polyamide 6 with very high rigidity and strength and light inherent color.

169707180

AKROTEK®

Preliminary

PK-VM GF 10 natural (8679)PK GF10

AKROTEK® PK-VM GF 10 natural (8679) is a 10% glass fibre reinforced Polyketone with average stiffness and strength. Due to its very good media resistance, the material is suitable for use in applications that carry cooling water. This type was developed as the successor to PK-VM GF 10 natural (8534) in order to meet the requirements for a larger processing window during processing.

Features

hydrolysis / chemically stabilised

Properties

Modulus

3.600MPa

Strength

75MPa

Impact

61kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
3600 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
75 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
9,3 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
61 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
205 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Humidity absorption

ISO 1110

70°C, 62% r.H.
0,7 - 0,8 %

Molding shrinkage

ISO 294-4

flow
transverse
0,6 - 0,8 %
1,3 - 1,5 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more