HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROLOY®

Preliminary

PA GF 30 black (6415)

PA66+PA6I/6T GF30

AKROLOY® PA GF 30 black (6415) is a 30% glass fibre reinforced, semi-aromatic polyamide blend with high stiffness and strength, even in conditioned state.


Modulus

9.800MPa

Strength

200MPa

Impact

65kJ/m²

AKROLOY® PA GF 30 black (6415) is a 30% glass fibre reinforced, semi-aromatic polyamide blend with high stiffness and strength, even in conditioned state.

AKROTEK®

PK-VM 8 black (6466)

PK

AKROTEK® PK-VM 8 black (6466) - Polyketon, Tribology, friction and wear, chemical resistance, food, drinking water, EU 10/2011


Modulus

1.600MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-VM 8 black (6466) - Polyketon, Tribology, friction and wear, chemical resistance, food, drinking water, EU 10/2011

AKROMID®

Preliminary

T5 8 black (6454)

PPA

AKROMID® T5 8 black (6454) - PPA, unreinforced, food contact, kitchen and household appliances, fitting, ACS, WRAS, NSF 61, EU 10/2011, FDA


Modulus

3.800MPa

Strength

75MPa

Impact

40kJ/m²

AKROMID® T5 8 black (6454) - PPA, unreinforced, food contact, kitchen and household appliances, fitting, ACS, WRAS, NSF 61, EU 10/2011, FDA

AKROMID®

Preliminary

B28 GF 15 natural (6940)

PA6 GF 15

AKROMID B28 GF 15 natural (6940) - PA 6, glass fiber reinforced, easy flow, good surface, bus fire standard ECE R 118.03, medium stiffness and strength.


Modulus

5.300MPa

Strength

120MPa

Impact

39kJ/m²

AKROMID B28 GF 15 natural (6940) - PA 6, glass fiber reinforced, easy flow, good surface, bus fire standard ECE R 118.03, medium stiffness and strength.

AKROTEK®

Preliminary

PK-VM GF 40 8 black (6995)

PK GF40

AKROTEK® PK-VM GF 40 8 black (6995) - Polyketon, 40% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

11.000MPa

Strength

150MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 40 8 black (6995) - Polyketon, 40% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)

PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.


Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

AKROMID®

A3 GF 50 4 natural (71090)

PA66 GF50

AKROMID® A3 GF 50 4 natural (71090) - PA6.6, 50% glass fiber, cooling water, hydrolysis resistant, DPPD free


Modulus

18.000MPa

Strength

260MPa

Impact

110kJ/m²

AKROMID® A3 GF 50 4 natural (71090) - PA6.6, 50% glass fiber, cooling water, hydrolysis resistant, DPPD free

168697080

AKROTEK®

PK-VM GF 10 grey (7344)PK GF10

AKROTEK® PK-VM GF 10 grey (7344) is a 10% glass fibre reinforced Polyketone with average stiffness and strength. The material is colored in grey similar to RAL 7044. This grade is suitable for parts of switches in the electric industry.

Features

hydrolysis / chemically stabilised

Properties

Modulus

3.600MPa

Strength

65MPa

Impact

50kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
3600 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
65 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
10 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
50 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
205 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

General properties


Density

ISO 1183

23°C
1,32 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
0,7 - 0,8 %

Molding shrinkage

ISO 294-4

flow
transverse
0,7 - 0,9 %
1,3 - 1,5 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.