AKROMID®

B3 GF 30 8 natural (5663)

PA6 GF30

AKROMID® B3 GF 30 8 natural (5663) - PA6, 30% glass fiber, food contact, kitchen and household appliances


Modulus

10.000MPa

Strength

185MPa

Impact

95kJ/m²

AKROMID® B3 GF 30 8 natural (5663) - PA6, 30% glass fiber, food contact, kitchen and household appliances

AKROTEK®

PK-HM 8 natural (6145)

PK

AKROTEK® PK-HM 8 natural (6145) - Polyketon, unreinforced, Tribology, friction and wear, chemical resistance, EU 10/2011, FDA 21 CFR


Modulus

1.400MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-HM 8 natural (6145) - Polyketon, unreinforced, Tribology, friction and wear, chemical resistance, EU 10/2011, FDA 21 CFR

AKROLOY®

Preliminary

PA GF 40 natural (6413)

PA66+PA6I/6T GF40

AKROLOY® PA GF 40 natural (6413) is a 40% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.


Modulus

13.000MPa

Strength

235MPa

Impact

95kJ/m²

AKROLOY® PA GF 40 natural (6413) is a 40% glass fibre reinforced, semi-aromatic polyamide blend with very high stiffness and strength, even in conditioned state.

AKROMID®

A3 5 black (4701)

PA66

AKROMID® A3 5 black (4701) is an unreinforced, high temperature stabilised polyamide 6.6


Modulus

3.500MPa

Strength

90MPa

Impact

180kJ/m²

AKROMID® A3 5 black (4701) is an unreinforced, high temperature stabilised polyamide 6.6

AKROMID®

Preliminary

B3 1 S3 natural (8013)

PA6-I

AKROMID® B3 1 S3 natural (8013) - PA 6 unreinforced, impact modified, connecting and fixing systems.


Modulus

2.200MPa

Strength

55MPa

Impact

180kJ/m²

AKROMID® B3 1 S3 natural (8013) - PA 6 unreinforced, impact modified, connecting and fixing systems.

AKROMID®

Preliminary

NEXT G3 GF 30 1 L CI natural (8377)

PA6.9 + PP GF30

AKROMID® NEXT G3 GF 30 1 L CI natural (8377) - PA 6.9/PP blend, bio-based, certified, low moisture absorption, weight reduction.


Modulus

8.000MPa

Strength

125MPa

Impact

65kJ/m²

AKROMID® NEXT G3 GF 30 1 L CI natural (8377) - PA 6.9/PP blend, bio-based, certified, low moisture absorption, weight reduction.

AKROTEK®

PK-HM 8 black (6246)

PK

AKROTEK® PK-HM 8 black (6246) is an unreinforced, high viscosity polyketone. The material is suitable for drinking water contact and meets the requirements according to ACS and WRAS. Moreover the material corresponds to the European food guideline EU 10/2011, but not to the American FDA 21 CFR.


Modulus

1.600MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-HM 8 black (6246) is an unreinforced, high viscosity polyketone. The material is suitable for drinking water contact and meets the requirements according to ACS and WRAS. Moreover the material corresponds to the European food guideline EU 10/2011, but not to the American FDA 21 CFR.

167686980

PRECITE®

Preliminary

E GF 50 natural (7300)PET GF50

PRECITE® E GF 50 natural (7300) is a 50% glass fibre reinforced, medium viscous polyethylene terephthalate (PET) with very high stiffness and toughness even at elevated temperatures. Due to its low moisture absorption, this material is particularly dimensionally stable and therefore perfectly suitable for precision parts in the automotive, E&E and household goods industries, where a very good surface finish is required.

Features

surface modified
reduced moisture
E&E
metal substitution
Sports & leisure

Properties

Modulus

18.100MPa

Strength

220MPa

Impact

70kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
18100 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
220 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
1,8 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
21000 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
350 MPa

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
30°C | d.a.m.
-
70 kJ/m²
50 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
30°C | d.a.m.
-
14 kJ/m²
14 kJ/m²

Izod impact strength

ISO 180/1A

23°C | d.a.m.
54 kJ/m²

Izod notched impact strength

ISO 180/1A

23°C | d.a.m.
11 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
235 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
250 °C

Coefficient of linear thermal expansion

ISO 11359-1/2

23°C to 80°C | parallel
23°C to 80°C | transverse
0,13 10⁻⁴/K
0,68 10⁻⁴/K

Flammability


Burning rate

UL 94

0,8 mm Wall thickness
HB Class

General properties


Density

ISO 1183

23°C
1,75 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,1 - 0,3 %
0,5 - 0,7 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more