C3 GF 60 1 black (4659)

PA66 + PA6 GF60

AKROMID® C3 GF 60 1 black (4659) is a 60% glass fibre reinforced, heat stabilised polyamide 6.6/6 - Blend.


Modulus

21.300MPa

Strength

270MPa

Impact

96kJ/m²

AKROMID® C3 GF 60 1 black (4659) is a 60% glass fibre reinforced, heat stabilised polyamide 6.6/6 - Blend.

AKROTEK®

PK-HM black (4953)

PK

AKROTEK® PK-HM black (4953) - Polyketon, Tribology, friction and wear, chemical resistance


Modulus

1.500MPa

Strength

60MPa

Impact

180kJ/m²

AKROTEK® PK-HM black (4953) - Polyketon, Tribology, friction and wear, chemical resistance

AKROTEK®

PK-VM GF 50 8 black (6936)

PK GF50

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

14.000MPa

Strength

170MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 50 8 black (6939) - Polyketon, 50% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

AKROTEK®

Preliminary

PK-VM GF 20 natural (6982)

PK GF20

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.


Modulus

5.800MPa

Strength

100MPa

Impact

50kJ/m²

AKROTEK® PK-VM GF 20 8 natural (6982) is a 20% glass fibre reinforced, low viscous polyketone with average stiffness and strength and light inherent color. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61 and does NOT correspond to the European food guideline EU 10/2011 as well as to the American FDA 21 CFR guideline.

AKROMID®

B3 GF 40 1 black (20016)

PA6 GF40

AKROMID® B3 GF 40 1 black (20016) is a 40% glass fibre reinforced, heat stabilised polyamide 6 with very high stiffness and strength


Modulus

12.500MPa

Strength

195MPa

Impact

95kJ/m²

AKROMID® B3 GF 40 1 black (20016) is a 40% glass fibre reinforced, heat stabilised polyamide 6 with very high stiffness and strength

AKROMID®

Preliminary

NEXT G3 GF 30 1 L CI natural (8377)

PA6.9 + PP GF30

AKROMID® NEXT G3 GF 30 1 L CI natural (8377) - PA 6.9/PP blend, bio-based, certified, low moisture absorption, weight reduction.


Modulus

8.000MPa

Strength

125MPa

Impact

65kJ/m²

AKROMID® NEXT G3 GF 30 1 L CI natural (8377) - PA 6.9/PP blend, bio-based, certified, low moisture absorption, weight reduction.

AKROMID®

B3 black (2502)

PA6

AKROMID® B3 black (2502) is an unreinforced polyamide 6.


Modulus

3.600MPa

Strength

85MPa

Impact

180kJ/m²

AKROMID® B3 black (2502) is an unreinforced polyamide 6.

164656680

AKROMID®

Preliminary

NEXT G3 GF 30 1 L CI natural (8377)PA6.9 + PP GF30

AKROMID® NEXT G3 GF 30 1 L CI natural (8377) is a 30% glass fiber reinforced PA 6.9/PP blend with high strength and stiffness. The partially bio-based grade is characterised by particularly low moisture absorption and high chemical resistance compared to classic PA 6 and PA 6.6. It is suitable for applications where weight reduction and sustainability are required. The material is certified according to ISCC PLUS. 34% of the fossil raw materials required for manufacturing this product were replaced by sustainable biomass-balanced PP (≙ allocation factor).

Features

biomass balanced
Bio-based
heat stabilised 130
reduced density
reduced moisture
E&E
Sports & leisure

Regulatory

iscc-plus

Properties

Modulus

8.000MPa

Strength

125MPa

Impact

65kJ/m²

Sustainability


Biobased carbon content

32 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
8000 MPa
7000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
125 MPa
110 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
3,1 %
4,0 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
65 kJ/m²
65 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
14,5 kJ/m²
15,0 kJ/m²

Thermal Properties


Melting temperature

ISO 11357-3

DSC, 10K/min
219 °C

General properties


Density

ISO 1183

23°C
1,23 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
0,7 - 0,9 %

Water absorption

ISO 62

23°C, saturated
2,0 - 2,4 %

Molding shrinkage

ISO 294-4

flow
transverse
0,1 - 0,3 %
0,6 - 0,8 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more