AKROMID®

Preliminary

S3 GF 30 4 black (3429)

PA610 GF30

AKROMID® S3 GF 30 4 black (3429) is a 30% glass fibre reinforced and hydrolysis stabilised polyamide 6.10 with high stiffness and strength as well as lower moisture absorption and very high chemical resistance.


Modulus

8.600MPa

Strength

160MPa

Impact

110kJ/m²

AKROMID® S3 GF 30 4 black (3429) is a 30% glass fibre reinforced and hydrolysis stabilised polyamide 6.10 with high stiffness and strength as well as lower moisture absorption and very high chemical resistance.

AKROMID®

A3 GK 30 natural (3689)

PA66 GB30

AKROMID® A3 GK 30 natural (3689) - PA 6.6, 30% glass beads reinforced, good surface, low warpage


Modulus

5.000MPa

Strength

90MPa

Impact

28kJ/m²

AKROMID® A3 GK 30 natural (3689) - PA 6.6, 30% glass beads reinforced, good surface, low warpage

AKROMID®

A3 1 L black (4652)

PA66 + PP

AKROMID® A3 1 L black (4652) - unreinforced PA6.6/PP-Blend lightweight, cost reduced


Modulus

2.300MPa

Strength

54MPa

Impact

180kJ/m²

AKROMID® A3 1 L black (4652) - unreinforced PA6.6/PP-Blend lightweight, cost reduced

AKROMID®

A3 1 L natural (4800)

PA66 + PP

AKROMID® A3 1 L natural (4800) - unreinforced PA6.6/PP-Blend lightweight, cost reduced


Modulus

2.300MPa

Strength

55MPa

Impact

180kJ/m²

AKROMID® A3 1 L natural (4800) - unreinforced PA6.6/PP-Blend lightweight, cost reduced

AKROLOY®

Preliminary

PA GF 30 black (6415)

PA66+PA6I/6T GF30

AKROLOY® PA GF 30 black (6415) is a 30% glass fibre reinforced, semi-aromatic polyamide blend with high stiffness and strength, even in conditioned state.


Modulus

9.800MPa

Strength

200MPa

Impact

65kJ/m²

AKROLOY® PA GF 30 black (6415) is a 30% glass fibre reinforced, semi-aromatic polyamide blend with high stiffness and strength, even in conditioned state.

AKROMID®

A3 GK 30 6 natural (6774)

PA66 GB30

AKROMID® A3 GK 30 6 natural (6774) - 30% glass bead, inorganic high temperature stabilised, polyamide 6.6, low warpage, high surface appearance


Modulus

4.600MPa

Strength

90MPa

Impact

25kJ/m²

AKROMID® A3 GK 30 6 natural (6774) - 30% glass bead, inorganic high temperature stabilised, polyamide 6.6, low warpage, high surface appearance

AKROTEK®

Preliminary

PK-VM GF 15 8 black (6991)

PK GF15

AKROTEK® PK-VM GF 15 8 black (6991) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA


Modulus

4.500MPa

Strength

95MPa

Impact

55kJ/m²

AKROTEK® PK-VM GF 15 8 black (6991) - Polyketon, 15% glass fiber, Tribology, friction and wear, chemical resistance, food contact, EU 10/2011, FDA

164656680

AKROMID®

B3 GFM 10/20 1 black (2017)PA6 (GF10+M20)

AKROMID® B3 GFM 10/20 1 black 950089 (2017) is a 10% glass fibre reinforced and 20% mineral filled, heat stabilised polyamide 6 with good surface and dimensional stability

Features

heat stabilised 130
surface modified
low warpage

Properties

Modulus

6.200MPa

Strength

110MPa

Impact

40kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
6200 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
110 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
3,5 %

Flexural modulus

ISO 178

2 mm/min | d.a.m.
4000 MPa

Flexural strength

ISO 178

2 mm/min | d.a.m.
170 MPa

Flexural strain at break

ISO 178

2 mm/min | d.a.m.
5,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
30°C | d.a.m.
-
40 kJ/m²
40 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
3 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
185 °C

Temperature of deflection under load HDT/B

ISO 75

0,45 MPa
215 °C

Temperature of deflection under load HDT/C

ISO 75

8 MPa
55 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
222 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,36 g/cm³

Molding shrinkage

ISO 294-4

flow
transverse
0,6 %
0,8 %

Rheological Properties


Flowability

AKRO

1 mm Thickness
2 mm Thickness
170 mm
390 mm

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more