558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROTEK®

Preliminary

PK-VM M 7 natural (8858)

PK M7

AKROTEK® PK-VM M 7 natural (8858) - 7 % mineral reinforced Polyketon, high flowability and good weldline perfomance.


Modulus

2.700MPa

Strength

65MPa

Impact

120kJ/m²

AKROTEK® PK-VM M 7 natural (8858) - 7 % mineral reinforced Polyketon, high flowability and good weldline perfomance.

AKROMID®

Preliminary

B3 GF 50 4 RM-M 2 black (8234)

PA6+X GF50

AKROMID® B3 GF 50 4 RM-M 2 black (8234) - 50% glass fiber reinforced PA 6 with good surface properties, UV stabilised, chemically stabilised, reduced moisture absorption


Modulus

16.800MPa

Strength

210MPa

Impact

50kJ/m²

AKROMID® B3 GF 50 4 RM-M 2 black (8234) - 50% glass fiber reinforced PA 6 with good surface properties, UV stabilised, chemically stabilised, reduced moisture absorption

AKROMID®

UL

A3 GF 35 1 HU black (8417)

PA66 GF35

AKROMID® A3 GF 35 1 HU black (8417) - PA 6.6, 35% glass fibre, heat ageing resistant, high rigidity and strength, very good flowability, UL listed HB.


Modulus

12.000MPa

Strength

215MPa

Impact

75kJ/m²

AKROMID® A3 GF 35 1 HU black (8417) - PA 6.6, 35% glass fibre, heat ageing resistant, high rigidity and strength, very good flowability, UL listed HB.

AKROMID®

Preliminary

C3 GF 30 1 natural (8574)

PA66 + PA6 GF30

AKROMID® C3 GF 30 1 natural (8574) - PA6.6/6 blend, 30% glass fiber reinforced, heat stabilised, industrial engineering, automotive industry


Modulus

9.300MPa

Strength

185MPa

Impact

75kJ/m²

AKROMID® C3 GF 30 1 natural (8574) - PA6.6/6 blend, 30% glass fiber reinforced, heat stabilised, industrial engineering, automotive industry

AKROMID®

Preliminary

T5 GF 40 6 natural (8003)

PPA GF40

AKROMID® T5 GF 40 6 natural (8003) - 40% glass fibre reinforced with high stiffness and strength, high temperature resistance, e.g. under the hood applications


Modulus

16.000MPa

Strength

245MPa

Impact

80kJ/m²

AKROMID® T5 GF 40 6 natural (8003) - 40% glass fibre reinforced with high stiffness and strength, high temperature resistance, e.g. under the hood applications

AKROTEK®

Preliminary

PK-VM GF 60 black (8689)

PK GF60

AKROTEK® PK-VM GF 60 black (8689)- Polyketon, 60% glass fibre reinforced, chemical and hydrolysis resistance


Modulus

16.700MPa

Strength

170MPa

Impact

60kJ/m²

AKROTEK® PK-VM GF 60 black (8689)- Polyketon, 60% glass fibre reinforced, chemical and hydrolysis resistance

AKROMID®

Preliminary

B3 GF 40 5 black (8726)

PA6 GF40

AKROMID® B3 GF 40 5 black (8726) - PA6, 40% GF, high heat stabilised, UV stabilised, technical parts in industrial engineering, automotive industry, agriculture.


Modulus

12.500MPa

Strength

200MPa

Impact

95kJ/m²

AKROMID® B3 GF 40 5 black (8726) - PA6, 40% GF, high heat stabilised, UV stabilised, technical parts in industrial engineering, automotive industry, agriculture.

154555680

AKROTEK®

Preliminary

PK-VM GF 10 8 natural (6981)PK GF10

AKROTEK® PK-VM GF 10 8 natural (6981) is a 10% glass fibre reinforced polyketone with average stiffness and strength. PK is characterized by its outstanding media resistance, which qualifies it to be used for components that are in contact with chemicals. The material corresponds to the European food guideline EU 10/2011 and to the American FDA 21 CFR. This grade is suitable for parts of kitchen and household appliances. Please note that the material is NOT suitable anymore for drinking water contact and does NOT meet the requirements according to KTW, DVGW W270, ACS, WRAS as well as NSF61.

Features

hydrolysis / chemically stabilised

Regulatory

eu102011fda

Properties

Modulus

3.700MPa

Strength

80MPa

Impact

50kJ/m²

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
3700 MPa
3600 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
80 MPa
80 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
4,2 %
4,2 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
50 kJ/m²
45 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
9 kJ/m²
9 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
205 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
220 °C

Flammability


Burning rate

UL 94

1,6 mm Wall thickness
HB Class

Burning rate (<100 mm/min)

FMVSS 302

> 1 mm Thickness
+

General properties


Density

ISO 1183

23°C
1,32 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
0,7 - 0,8 %

Molding shrinkage

ISO 294-4

flow
transverse
0,7 - 0,9 %
1,3 - 1,5 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.

Learn more