HEADER Granulat 1920x700

Find the right compound

Select your fitting and find the right compound for your intend

Tensile Modulusin MPa
Tensile Strengthin MPa
Charpy impact strengthin kJ/m²
558 Compounds found
Recommended  
Tensile Modulus
Tensile Strength
Charpy impact strength
Description

AKROTEK®

UL
Preliminary

PK-VM GF 30 FR orange (8537)

PK GF30 FR(40)

AKROTEK® PK-VM GF 30 FR orange (8537) - Polyketon, 30% GF, chemical and hydrolysis resistance, flame retardant, halogenefree, orange RAL 2003, process improved, good dimensional stability. high voltage components, e-mobility.


Modulus

8.600MPa

Strength

125MPa

Impact

70kJ/m²

AKROTEK® PK-VM GF 30 FR orange (8537) - Polyketon, 30% GF, chemical and hydrolysis resistance, flame retardant, halogenefree, orange RAL 2003, process improved, good dimensional stability. high voltage components, e-mobility.

PRECITE®

Preliminary

P3 GF 30 4 LA black (8286)

PBT-I GF30

PRECITE®P3 GF 30 4 LA black (8286) PBT, 30% GF, hydrolysis stabilised, laser markable high stiffness, high toughness, GMA free, low moisture absorption, dimensional stability, light black


Modulus

9.100MPa

Strength

120MPa

Impact

70kJ/m²

PRECITE®P3 GF 30 4 LA black (8286) PBT, 30% GF, hydrolysis stabilised, laser markable high stiffness, high toughness, GMA free, low moisture absorption, dimensional stability, light black

AKROMID®

UL

C3 GF 30 1 FR black (7243)

PA66+PA6 GF30 FR(40)

AKROMID® C3 GF 30 1 FR black (7243) - PA6/6.6 blend, 30 % glass fiber, flame retardant, good flowability, UL-listed, E&E, Public transportation EN 45545-2.


Modulus

10.800MPa

Strength

148MPa

Impact

74kJ/m²

AKROMID® C3 GF 30 1 FR black (7243) - PA6/6.6 blend, 30 % glass fiber, flame retardant, good flowability, UL-listed, E&E, Public transportation EN 45545-2.

AKROMID®

UL

C3 GF 25 1 FR black (7246)

PA66+PA6 GF25 FR(40)

AKROMID® C3 GF 25 1 FR black (7246) - PA6/6.6 blend, 25% glass fiber, flame retardant, good flowability, high strength, UL-listed, automotive, E&E market.


Modulus

9.100MPa

Strength

137MPa

Impact

66kJ/m²

AKROMID® C3 GF 25 1 FR black (7246) - PA6/6.6 blend, 25% glass fiber, flame retardant, good flowability, high strength, UL-listed, automotive, E&E market.

AKROLOY®

UL

PA GF 50 HU black (8198)

PA66+PA6I/6T GF50

AKROLOY® PA GF 50 HU black (8198) is an UL listed, 50% glass fibre reinforced, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.


Modulus

17.000MPa

Strength

265MPa

Impact

105kJ/m²

AKROLOY® PA GF 50 HU black (8198) is an UL listed, 50% glass fibre reinforced, semi-aromatic polyamide-blend with very high stiffness and strength, even in conditioned state.

AKROMID®

UL

C3 GF 25 1 FR natural (7208)

PA66+PA6 GF25 FR(40)

AKROMID® C3 GF 25 1 FR natural (7208) - PA6/6.6 blend, 25% glass fiber, flame retardant, good flowability, high strength, UL-listed, automotive, E&E market.


Modulus

9.200MPa

Strength

140MPa

Impact

73kJ/m²

AKROMID® C3 GF 25 1 FR natural (7208) - PA6/6.6 blend, 25% glass fiber, flame retardant, good flowability, high strength, UL-listed, automotive, E&E market.

AKROMID®

UL
Preliminary

C3 GF 30 1 FR grey (8384)

PA66+PA6 GF30 FR(40)

AKROMID® C3 GF 30 1 FR grey (8384) - PA6/6.6 blend, 30 % glass fiber, flame retardant, good flowability, UL-listed, RAL 7035, E&E, Public transportation EN 45545-2.


Modulus

10.000MPa

Strength

121MPa

Impact

46kJ/m²

AKROMID® C3 GF 30 1 FR grey (8384) - PA6/6.6 blend, 30 % glass fiber, flame retardant, good flowability, UL-listed, RAL 7035, E&E, Public transportation EN 45545-2.

123480

AKROMID®

Preliminary

NEXT 5.10 3 GF 30 natural (8406)PA5.10 GF30

The biobased AKROMID® NEXT 5.10 3 GF 30 natural (8406) is a HMD-free (hexamethylenediamine) alternative to PA 6.10. With 30% glass fibre reinforcement, the material is suitable for components with high strength requirements.

Features

heat stabilised 130
electrically neutral

Properties

Modulus

8.300MPa

Strength

160MPa

Impact

72kJ/m²

Sustainability


Biobased carbon content

97 %

Mechanical Properties


Tensile modulus

ISO 527-2

1 mm/min | d.a.m.
1 mm/min | conditioned
8300 MPa
6000 MPa

Tensile stress at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
160 MPa
120 MPa

Tensile strain at break

ISO 527-2

5 mm/min | d.a.m.
5 mm/min | conditioned
3,2 %
4,5 %

Charpy impact strength

ISO 179-1/1eU

23°C | d.a.m.
23°C | conditioned
72 kJ/m²
74 kJ/m²

Charpy notched impact strength

ISO 179-1/1eA

23°C | d.a.m.
23°C | conditioned
13 kJ/m²
14 kJ/m²

Thermal Properties


Temperature of deflection under load HDT/A

ISO 75

1,8 MPa
194 °C

Melting temperature

ISO 11357-3

DSC, 10K/min
217 °C

General properties


Density

ISO 1183

23°C
1,29 g/cm³

Humidity absorption

ISO 1110

70°C, 62% r.H.
1,2 %

Disclaimer

All specifications and information given on this website are based on our current knowledge and experience. A legally binding promise of certain characteristics or suitability for a concrete individual case cannot be derived from this information. The information supplied here is not intended to release processors and users from the responsibility of carrying out their own tests and inspections in each concrete individual case. AKRO®, AKROMID®, AKROLEN®, AKROLOY®, AKROTEK®, ICX® and PRECITE® are registered trademarks of the Feddersen Group.

Contact

Do you have any questions? We are happy to help.

Would you like to learn more about AKRO-PLASTIC GmbH? Contact us! We will be happy to help you.